Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.00 - 3.60 g/cc | 3.00 - 3.60 g/cc | |
Parker Chomerics CHO-BOND SV712 Conductive Epoxy CHO-BOND® 700 Series Adhesives for Microelectronics Packaging; these pure silver-filled epoxy pastes are designed to meet the demanding requirements of semiconductor and microelectronic packaging. .. |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 9H0300C LNP* Thermocomp* 9H0300C is a High Specific Gravity compound containing proprietary fillers. |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | |
Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating Master Bond MB600SCN is an aqueous based, sodium silicate system with a silver coated nickel filler. It is intended for use in applications where very good shielding effectiveness is required and co.. |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | |
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator Fibermax Mat is a high-temperature, flexible mat product that is lightweight (1.5 lb/ft3 density) and highly resilient. It is composed entirely of Fibermax polycrystalline mullite fibers to produce.. |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | |
Unifrax Fibermax® Needled Blanket Fibermax® Needled Blankets are high temperature, light weight and flexible products manufactured from polycrystalline mullite fiber that can be exposed to temperatures up to 1600°C (2912°F). Fib.. |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | Mixed, degassed |
Tra-Con Tra-Duct 29121 Snap Cure Conductive Silver Epoxy Adhesive TRA-DUCT 29121 is 100% solids, two component silver filled epoxy designed for chip bonding in microelectronic and optoelectronic applications. TRA-DUCT 29121 is a soft, smooth paste. This two-part f.. |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | |
Unifrax Fiberfrax® Fibermax Bulk Mullite High-Temperature Fiber In addition to Fiberfrax Bulk Fibers, Unifrax has the ability to produce many different specialty fibers that provide a variety of desirable performance properties for certain applications. These f.. |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | at 25°C |
Daikin DAI-EL G-952 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 69% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good solvent resistance and low-temperature characteristics.Information provided by Daikin Industrie.. |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | ISO 1183 |
Ecomass® 705ZC75 Stainless Steel Filled ABS Nontoxic Alternative to traditional metals, weighting and balancing applicationsModerate Specific GravityStainless Steel Powder Filled ABSInformation provided by Technical Polymers |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | ISO 1183 |
Ecomass® 705ZD70 Tungsten Filled ABS Nontoxic Alternative to Lead (Pb) for radiation shielding applicationsHigh specific GravityTungsten Filled ABS compoundRigidGood ToughnessInformation provided by Technical Polymers |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | |
Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina Good corrosion electrical and thermal shock resistance. Plates from 1/4" to 3/4" thick; rods from 1/4" to 3" diameter. Easily machined using conventional tools, no firing required. |
|||
Specific Gravity | 3.00 g/cc | 3.00 g/cc | |
Aremco AREMCOLOX™ 502-400 Machinable Glass Ceramic High dielectric and mechanical strength. For high voltage insulators, coil forms, soldering fixtures, arc barriers. Readily machined, no firing required. Plates from 1/8" to 1" thick; rods from 1.. |