Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.0040 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Plastcom SLOVAMID 6/66 GF 50 PA6/66, 50% glass fibre
FeaturesPA 6/66 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-g..
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
With Flow; ISO 2577
Polykemi AB SCANAMID 66 A43^E F14 Nylon 66, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Ineos Nova 765 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High flow, High impact, Color stable, Custom colorsApplications: High flow, multi-purpose injection molding grade where color stability is a requirement, Toys, Appliance, Computer peripheralsPerform..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Ineos Nova Zyntar® 7001 High Performance Flame Retardant Polystyrene  (discontinued **)
Super high flow, Reduced processing temperatures, Reduced processing time, Improved aesthetics, Custom colorsApplications: Injection molding, Gas-assist injection molding, Hard to fill cavities, suc..
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Compression; ASTM D955
Plenco 306 Black General Purpose Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 306 is a two-stage, mineral and flock-filled phenolic molding compound designed to have the heat resistant characteristics of Plaslok 504, while at the same time, improved impact strength.Da..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Internal; 50x50mm
SYNTHOS Forsan® 393 Acrylonitrile Butadiene Styrene (ABS)
High heat resistance, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Ka..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ISO 294-4
Styrolution PS 124 N/L GPPS
Styrolution PS 124N/L is a general purpose polystyrene grade with a good flow characteristic and an improved heat resistance.Excellent flow propertiesHigh heat resistanceUL 94 HB (Antwerp only)Infor..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D 955
Styrolution PS 2600/2601 GPPS
Foam extrusionLow residual styrene monomer contentModerate heat resistanceGood balance of strength and ease of processingUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolut..
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene
Saxalac 310A is a medium viscosity, impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
PlastxWorld CEVIAN® S1100 High Impact PC/ABS alloy
These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Total PSI 7240 High Impact Polystyrene
7240 is a very high impact polystyrene for the extrusion industry. This grade has been designed to be diluted with crystal polystyrene (such as LACQRENE® 140, 1340 or 1540) at higher levels than c..
Linear Mold Shrinkage 0.0040 cm/cm

@Thickness 3.175 mm
0.0040 in/in

@Thickness 0.1250 in
ASTM D955
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Diamond Polymers ABS 3500ELG
Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Diamond Polymers ABS 4000HH
Description: Heat Resistant Grade, Medium High HeatInformation provided by Diamond Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Diamond Polymers ASA/PC TA-35
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Americas Styrenics MC3650 High Heat Crystal Polystyrene
Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer..
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Test Box 1.5 mm
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Linear Mold Shrinkage 0.0040 - 0.0090 cm/cm
0.0040 - 0.0090 in/in
ASTM D955
Asia International Enterprise (Hong Kong) 60G5F Nylon 66, 25% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D-955
Bhansali Engineering Abstron HI-40 ABS High Impact Injection Molding
Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D-955
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade
Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Total Lacqrene® 6630 Impact Polystyrene  (discontinued **)
LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ISO D955
Ineos Nova 201 Crystal Polystyrene High Heat Extrusion Grade  (discontinued **)
Excellent heat resistance, Superior melt strengthApplications: Foam insulation, Oriented polystyrene sheet (OPS), XPS food packaging, Sheet and profile extrusionProperties were determined on injecti..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
PlastxWorld CEVIAN® B2704 20% GF PBT/ABS Alloy
Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Kleerdex Kydex® 1900 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Mid-temperature aircraft gradeApplications: This sheet product is designed for use in small aircraft interiors but also is appropriate for other applications where higher in-service temperatures may..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Ineos Nova 5530 High Impact Polystyrene  (discontinued **)
Good overall balance of properties, Good toughnessApplications: Audio cassettes and cartridges, Housewares, Toys, Industrial productsProperties were determined on injection molded specimens at 23°C..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Ineos Nova 1204 High Heat Crystal Polystyrene
Good processing characteristics, High tensile strength and modulus, Excellent clarity, USP Class VIApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radia..
Copyright © lookpolymers.com All Rights Reserved