Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.0040 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
STN EN ISO 294-4
Plastcom SLOVAMID® 6 GF 35 LS PA6 reinforced with glass fiber, UV stabilized
PA 6 for injection molding, reinforced with 35% glass fiber, UV stabilized, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools..
Linear Mold Shrinkage 0.0040 cm/cm

@Thickness 3.20 mm
0.0040 in/in

@Thickness 0.126 in
ASTM D 955
RTP Company RTP 4099 X 117359 D Polyphthalamide (PPA) LDS Platable - Glass Fiber - Mineral
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Ineos Nova 1511 High Heat Crystal Polystyrene  (discontinued **)
High flow and high heat resistance, Excellent clarity, USP Class VIApplications: Injection moldingExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm

@Temperature 23.0 °C
0.0040 - 0.0060 in/in

@Temperature 73.4 °F
ASTM D955
Kingfa JH960 6610 Non-halogenated Flame Retardant PC/ABS Alloy
Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ISO 2577
LG Chemical LG-709 ABS, Low Gloss, Super High Heat Resistance
Information Provided by LG Chem
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Lehmann & Voss LUVOCOM® 1105-8001 PEEK, with glass spheres
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par..
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Spartech Royalite R61M Low Smoke Resin
Data provided by the manufacturer. Formulated to meet smoke and fire specifications recommended by the FTA, this is ideally suited for mass transit applications such as seat backs, overhead storage..
Linear Mold Shrinkage 0.0040 cm/cm

@Thickness 3.17 mm
0.0040 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Plaslube® J-50/10/SI/2 Polycarbonate, 10% GFR, 2% Silicone
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene
POLYSTYRENE IMPACT 3450 is a high impact polystyrene with high heat resistance, good flow, high stiffness and good aesthetics. With such an ideal balance of properties, POLYSTYRENE IMPACT 3450 is w..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm

@Thickness 3.17 mm
0.0040 - 0.0070 in/in

@Thickness 0.125 in
ASTM D955
RTP Company PermaStat® 1800 A FR Polycarbonate/Acrylic Alloy (PC/PMMA), Flame Retardant - Permanently Anti-static - ESD Protection - UL94 V-0
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Total PSC 1960N Crystal Polystyrene
1960N is a high resistance crystal polystyrene with very high flow for the production of thick insulation board. The very low viscosity of this grade makes it particularly suitable for the producti..
Linear Mold Shrinkage 0.0040 - 0.010 cm/cm

@Thickness 3.17 mm
0.0040 - 0.010 in/in

@Thickness 0.125 in
ASTM D955
RTP Company RTP 101 CC TFE 10 Polypropylene (PP), Glass Fiber - Chemically Coupled - PTFE Lubricated
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D 955
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Diamond Polymers ABS 2100 P Compounding Grade Powder
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Diamond Polymers ABS 3003MC Black 1722
Description: BlackInformation provided by Diamond Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Diamond Polymers ABS 3501 Natural 1050
Description: Natural, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Diamond Polymers ABS 7600B (ELG)
Description: Blow Molding Grade, Extra High Impact, Low GlossInformation provided by Diamond Polymers, Inc.
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Diamond Polymers NPP 60-1300 GF30 30% Glass Filled Polyester Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Diamond Polymers SE 3 HH
Description: High Heat ABSInformation provided by Diamond Polymers, Inc.
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Diamond Polymers ABSPC 7801E ABS/PC Extrusion Grade, High Impact, High Heat
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
MD; ASTM D955
Aclo Accutech Polypropylene Homopolymer HP0334G10CL Glass Reinforced Coupled
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D-955
Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene
Product CharacteristicsAdditive freeTypical ApplicationsFoamsFilms/opticalCarrier resinSpecialty blendingInformation provided by AmericasStyrenics LLC.
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
A. Schulman ComAlloy Voloy® 113 Polypropylene, Glass Reinforced, Chemically Coupled, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.25% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM Data MD
BASF Capron® 8332G Impact Modified, 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8332G is a 25% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of ..
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Total Lacqrene® 851 High Impact Polystyrene  (discontinued **)
LACQRENE® 851 is a flame retardant, high impact polystyrene, halogen free rated UL 94 V0 @ 2.5 mm and UL 94 5VA @ 2mm. LACQRENE® 851 offers rheological and mechanics properties which permits larg..
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene  (discontinued **)
Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po..
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Ineos Nova 207 Crystal Polystyrene High Heat, High Flow Grade  (discontinued **)
Fast cycling, Excellent flow characteristics, Extrusion and Injection Molding Applications: XPS sheet, Foam insulation, CD and DVD jewel boxesProperties were determined on injection molded specimen..
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D955
PolyOne Edgetek® PI-10GF/000 Polyetherimide (PEI), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Copyright © lookpolymers.com All Rights Reserved