Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ecomass® 3620BX60 18% Borated Polyethylene (HDPE)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ecomass® 3620BX60 18% Borated Polyethylene (HDPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
18% Borated Polyethylene (HDPE), Product Form - Pellets, No Pre-Drying RequiredProcessing Method: Injection Molding, Compression MoldingNeutron Shielding ApplicationsInformation provided by Technical Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
ASTM D638
Flexural Strength 13.8 MPa
2000 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.7 °C
170 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C
150 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 177 - 227 °C
350 - 440 °F
Mold Temperature 21.1 - 65.6 °C
70.0 - 150 °F