Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Mold Temperature | 21.1 - 71.1 °C | 70.0 - 160 °F | |
Northstar Polymers MPA-A30B Mold-Making Resin MPA-A30B is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPC-W44A Polyurethane Gel MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Mold Temperature | 21.1 - 29.4 °C | 70.0 - 85.0 °F | |
Northstar Polymers MPP-F07A Easy Hand-Mixable/Pourable Flexible Foam This foam formulation is designed to make molded flexible foam parts/sheets/dies/blocks by hand-mixing with very basic tools such as a cup and stir stick. The components are low-viscosity stable li.. |
|||
Mold Temperature | 21.1 - 93.3 °C | 70.0 - 200 °F | |
PTS Trimid® N6-200L Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 6003-45A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 6003-55A Z Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 6003-75A Specialty Thermoplastic Elastomer, Bondable to PC/PMMA, PC/PBT |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
RTP Company RTP 700 AR 15 TFE 15 High Density Polyethylene (HDPE), Aramid Fiber Reinforced - PTFE Lubricated |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
RTP Company RTP 701 High Density Polyethylene (HDPE), Glass Fiber |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
RTP Company RTP 705 High Density Polyethylene (HDPE), Glass Fiber |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
RTP Company RTP 799 X 50492 L Low Density Polyethylene (LDPE), Electrically Conductive |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add.. |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
RTP Company ESD C 780 High Density Polyethylene (HDPE), Carbon Fiber - ESD Protection - Electrically Conductive |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
RTP Company RTP 1500.5-50D Polyether-Ester Block Copolymer (TEEE / COPE), Glass Fiber |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 1500-40D UV NATURAL Polyether-Ester Block Copolymer (TEEE / COPE), UV Stabilized |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 1500-82D TFE 15 Polyether-Ester Block Copolymer (TEEE / COPE), PTFE Lubricated - Preliminary Data |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company PermaStat® 1500-50D Polyether-Ester Block Copolymer (TEEE/COPE), Permanently Anti-static - ESD Protection |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
Ecomass® 3608TU96 Tungsten Filled Polyethylene Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyethylene (HDPE)Information provided by Technical Polymers |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® 8068N Thermoplastic Elastomer Elastocon® 8068N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8068N is FDA compliant and well suited.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® 8078B Thermoplastic Elastomer Elastocon® 8078B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078B is well suited for consumer goods a.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® 8078NL Thermoplastic Elastomer Elastocon® 8078NL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a scratch and mar resistant surface finish. Elastocon® 8078NL is FDA c.. |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® CLR45 Thermoplastic Elastomer Elastocon® CLR45 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR45 is.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® CLR75 Thermoplastic Elastomer Elastocon® CLR75 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, non-blooming high strength properties and a tactile surface fin.. |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 6042-60A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested |