Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-D80B Rigid Polyurethane MPP-D80B has a high load-bearing property at hardness 80 D Durometer. This material has a relatively slow curing pattern. Whereas many polyurethane formulations of this hardness cure very fast thus.. |
|||
Mold Temperature | 21.1 - 93.3 °C | 70.0 - 200 °F | |
PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 6003-45A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 6042-50A Specialty Thermoplastic Elastomer, PC/ABS Bondable |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 6042-60A Z Specialty Thermoplastic Elastomer |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 6042-70A MD NATURAL Specialty Thermoplastic Elastomer; ISO 10993 Tested |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 6042-70A Specialty Thermoplastic Elastomer, PC/ABS Bondable |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
RTP Company RTP 700 FR High Density Polyethylene (HDPE), Flame Retardant RTP 700 FR is characterized by V-0 performance, good melt flow and outstanding fatigue resistance. |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
RTP Company RTP 703 High Density Polyethylene (HDPE), Glass Fiber |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
RTP Company RTP 799 X 50492 L Low Density Polyethylene (LDPE), Electrically Conductive |
|||
Mold Temperature | 21.1 - 93.3 °C | 70.0 - 200 °F | |
PTS Trimid® N6-G33L 33% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 1500-40D Polyether-Ester Block Copolymer (TEEE / COPE) |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 1500-40D UV NATURAL Polyether-Ester Block Copolymer (TEEE / COPE), UV Stabilized |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 1500-55D TFE 15 Polyether-Ester Block Copolymer (TEEE / COPE), PTFE Lubricated |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
RTP Company RTP 1501-55D Polyether-Ester Block Copolymer (TEEE/COPE), Glass Fiber |
|||
Mold Temperature | 21.1 - 60.0 °C | 70.0 - 140 °F | |
RTP Company RTP 2799 S X 118623 B Saturated Styrenic Block Copolymer, EMI/RFI Shielding |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® 2865PE Thermoplastic Elastomer Elastocon® 2865PE thermoplastic elastomer has been developed for applications that require rubber-like properties and a good surface finish. Elastocon® 2865PE is FDA compliant and well suited for.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui.. |
|||
Mold Temperature | 21.1 - 65.6 °C | 70.0 - 150 °F | |
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Clariant Renol TES3050A Thermoplastic Elastomer Alloy Data provided by Clariant Masterbatches |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer Elastocon® CLR40 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR40 is.. |
|||
Mold Temperature | 21.1 - 37.8 °C | 70.0 - 100 °F | |
Elastocon TPE Technologies Elastocon® CLR65 Thermoplastic Elastomer Elastocon® CLR65 is a transparent thermoplastic elastomer that has been developed for applications that require oil/plasticizer free, high strength properties and a tactile surface finish. Elastoc.. |
|||
Mold Temperature | 21.1 - 48.9 °C | 70.0 - 120 °F | |
RTP Company RTP 6042-50A UV BLACK Specialty Thermoplastic Elastomer, UV Stabilized - Bondable to ABS, PC, PC Alloys, PBT, RTPU |