Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
PolyOne Geon™ Vinyl Wire & Cable EMB405LU Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid)
Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: ..
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Quantum PPS
Information provided by Quantum Advanced Engineering Plastics
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Parker Chomerics V-THERM™ Thermally Conductive Elastomer
V-THERM thermally conductive elastomer interface pads are designed for use between heat generating components and cooling devices. This material conforms to surface irregularities under moderate app..
Specific Gravity 1.35 g/cc
1.35 g/cc
Radici Radilon® S CP300 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Specific Gravity 1.35 g/cc
1.35 g/cc
±0.03; DIN 53479
PolyOne Bergamid™ B70 G30 grey VN7445CF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible R5145B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Polymer Resources NY66-IM1-G33 Nylon 66, 33% Glass Reinforced, Toughened
Nylon 66, 33% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible B80MB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1850-8322 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1105-8184 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann..
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp DFZ22E PC
LNP* Thermocomp* DFZ22E is a compound based on Polycarbonate with Glass and Milled Fiber. Characteristics of this products is Easy Molding.This data was supplied by SABIC-IP for the Americas region..
Specific Gravity 1.35 g/cc
1.35 g/cc
23°C; ASTM D792
Teknor Apex APEX® 3310-65 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Specific Gravity 1.35 g/cc
1.35 g/cc
23°C; ASTM D792
Teknor Apex APEX® 3310-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med..
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Teknor Apex APEX® 80-C118Q Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Teknor Apex APEX® 1011 Polyvinyl Chloride, Semi-Rigid
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D 792
RTP Company EMI 330 D FR Polycarbonate (PC), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D 792
RTP Company RTP 200 D FR Nylon 6/12 (PA), Unreinforced - Flame Retardant
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Cheng Yu Plastic NG1250S Nylon 66, 25% Glass Fiber Reinforced
Specific Gravity 1.35 g/cc
1.35 g/cc
silicone property; Arlon SQA-TMS-024
Arlon 55106R028 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Specific Gravity 1.35 g/cc
1.35 g/cc
23°C; ASTM D792
Teknor Apex APEX® 3210-75 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
RTP Company RTP 205D MS UV  Nylon 6/12 (PA 6/12) Glass Fiber 30% - Molybdenum Disulfide - UV Stable &
Glass Fiber 30% - Molybdenum Disulfide - UV StableComments:Glass FiberMolybdenum DisulfideUV StabilizedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments..
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
PolyOne Geon™ Vinyl Wire & Cable JA508AF Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D-792
Axiall 2651 Rigid PVC, Molding
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D 792
RTP Company RTP 399 X 101161 Polycarbonate (PC), Carbon Fiber - Glass Fiber
Specific Gravity 1.35 - 1.40 g/cc
1.35 - 1.40 g/cc
ASTM D792
Spartech Royalite R60-LS (R61) PVC/Acrylic Fire Rated Sheet
Description: Fire Rated SheetInformation provided by Spartech.
Specific Gravity 1.35 - 1.39 g/cc
1.35 - 1.39 g/cc
ASTM D792
Compuestos Dominicanos Polycom AM-440495 PVC Compound
The polycom AM series are designed for the covering of wires for the production of fences. They are available in different colors and all provide excellent UV light and microorganisms resistance. A..
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Oxford Polymers 20GF 20% Glass Fiber Filled Polycarbonate for Injection Molding
20% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers.