Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.07 GPa | 300 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific) ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | 2.0 in/min; 0.125" thickness; ASTM D-638 |
Chevron Phillips MD6800 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Displays and retail product shelvingDurable household applicationsThin to medium thickness parts that require a combination of high flow and good.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D638 |
Spartech Sta-Tuf High Impact Thermoplastic Alloy Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | Type I, 51 mm/min; ASTM D638 |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM Data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.07 - 2.41 GPa | 300 - 350 ksi | |
Master Bond EP21LVMed Two Component, Low Viscosity USP Class VI Epoxy Master Bond EP21LVMed is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is formulated to cure readily at room tempera.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | |
Plastcom SLOVALEN PH 61 GB 30 PP, 30% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Tensile Modulus | 2.07 - 2.41 GPa | 300 - 350 ksi | ASTM D790 |
Alcoa KAMA 1500 Freezer Modified OPS
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | ASTM Data |
Styron Magnum™ 4435 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Tensile Modulus | 2.07 GPa | 300 ksi | TM R050-36 |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |