Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
NYCOA ASN 27 300 KNF 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6 Resin NYCOA ASN 27 300 KNF is a 30% glass fiber reinforced, heat stabilized Nylon 6 resin used for injection molding. This grade features excellent strength and stiffness, dimensional stability, and a gre.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R5145B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
Ravago Manufacturing Americas Enviramid™ N1335STHL BK Post Consumer Recycle Nylon 66, 35% Glass Filled Superior Toughness, Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7786 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Emergency running property.Improved wear behaviour, low warpage.High chemical resistance p.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP322 Cotton Fabric Description: Linen phenolic laminate with molybdenum disulfide. Provides the same lubricity as NP313, but has better machining qualities. Mechanical strength similar to, but slightly less than NP320.. |
|||
Specific Gravity | 1.35 - 1.45 g/cc @Thickness 1.57 mm |
1.35 - 1.45 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP634 Laminate Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Gromax BFG30-FH00N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.35 - 1.41 g/cc | 1.35 - 1.41 g/cc | ASTM D 792 |
Karina 752D48/1-C-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.35 - 1.41 g/cc | 1.35 - 1.41 g/cc | ASTM D 792 |
Karina E 846-10/189-IS-SD White PVC Compound Packaging Grade PVCInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Gromax BFG30-AS00N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ISO 1183 |
Gromax BFG30-AS00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.35 - 1.41 g/cc | 1.35 - 1.41 g/cc | ASTM D 792 |
Karina E 847-10/189-IS-SD White PVC Compound White PVC Compound for extrusion of films/SheetInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | |
Sylvin Technologies 9915-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific) 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
Teknor Apex APEX® 84468 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; Good UV Resistance Uses: Cable Jacketing; Insulation Forms: Pellets Agency Ratings: UL 1063; UL 1581; UL 62Information Provided by T.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
Teknor Apex Chemlon® 233 GI Nylon 6, 33% Glass Fiber Reinforced Features: High Impact, 33% Glass Reinforced; Highly toughened compound exhibiting strength and rigidity; Good Creep Resistance; Good Stiffness; Good Toughness; Impact Modified Processing Method: Inj.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp ZM3242 PPE+PS (Asia Pacific) Modified PPO* 30% mineral filled products, Non Halogenated Flame Retardant V-1 products.Supper low warpage series, HDT 110degCThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D 792 |
RTP Company ESD C 204 Nylon 6/6 (PA), Glass Fiber - Electrically Conductive - ESD Protection |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D 792 |
RTP Company RTP 1000 HI FR A Polybutylene Terephthalate (PBT), Impact Modified - Flame Retardant |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | |
Epoxy Technology EPO-TEK® M10-D Epoxy Paste Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
Colorite Polymers CS1535UL Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | silicone property; Arlon SQA-TMS-024 |
Arlon 55143R060 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: cured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Specific Gravity | 1.35 - 1.39 g/cc | 1.35 - 1.39 g/cc | ASTM D-792 |
Axiall 16780 Wire & Cable Flexible PVC 90C matte finish, vinyl elastomer.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
RTP Company RTP 200D FR Nylon 6/12 (PA 6/12) Flame Retardant
(discontinued **) Flame RetardantComments:Flame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data .. |
|||
Specific Gravity | 1.35 g/cc | 1.35 g/cc | ASTM D792 |
RTP Company RTP 2282 Polyetheretherketone (PEEK) Carbon Fiber 15%
(discontinued **) Carbon Fiber 15%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo.. |