Mechanical Properties Metric English Comments
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural
Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Oxford Polymers 10GF 10% Glass Fiber Reinforced ABS, Flame Retardant
10% Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers.
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
RedEye On Demand ABS for Rapid Prototyping
ABS or Acrylonitrile butadiene styrene is a true industrial thermoplastic that is impact-resistant and structurally strong. ABS parts are built with a layered manufacturing process utilizing Fused D..
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 1.07 J/cm

@Temperature 23.0 °C
2.00 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 1.07 J/cm

@Diameter 3.17 mm
2.00 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
BP Amoco Acclear® 8249 Random Copolymer Polypropylene, High Clarity Grade  (discontinued **)
Suggested fabrication methods: Sheet extrusion; Thermoforming; Extrusion, injection, stretch blow moldingFeatures: Ultra high clarity, Good impact, Excellent static controlComplies with FDA specific..
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
at 73°F; ASTM D256
M. Holland Company CP500 Polypropylene Copolymer
Features: High Flow, High Impact Resistance, Good StiffnessUses: Automotive, Interior Parts Closures, Household Goods, ToysApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformati..
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Ineos HP55-25-155 HDPE
A high performance high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blowmolding equipment, specifically where applications require ex..
Izod Impact, Notched 1.07 J/cm

@Temperature 22.8 °C
2.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled
30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc.
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PC GF10 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PEEK CF20 TL15 HF 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: High Flow and LubricatedInformation provided by TP Composi..
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Statiblend® 02036 Polypropylene
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PBT G/CF30 15% Glass/Carbon Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 15% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Westlake Plastics Tempalux® 30% GF Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad ..
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene
DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat..
Izod Impact, Notched 1.07 J/cm

@Thickness 3.20 mm
2.00 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 199 X 129987 B Polypropylene (PP) Glass Fiber - Chemically Coupled - Flame Retardant - Non PBB/PBDE
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
At 73°F; ASTM D256
Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate
Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar..
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Ecomass® 1003TU96 Tungsten Filled COPA
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by..
Izod Impact, Notched 1.07 J/cm

@Temperature 22.8 °C
2.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant Renol PA223G13 Nylon 6, 13% Glass Fiber, Impact Modified
Data provided by Clariant Masterbatches
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Asahi Kasei Thermylon® NSG-440A-H 60% Ceramic and Glass Fiber Reinforced
Information provided by Asahi Thermofil
Izod Impact, Notched 1.07 J/cm

@Temperature -40.0 °C
2.00 ft-lb/in

@Temperature -40.0 °F
ASTM Test
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 528L-33G Nylon 66, 33% Glass Reinforced
General purpose glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufactur..
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
Atom Adhesives AA-BOND 2110 Epoxy Adhesive
AA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, no..
Izod Impact, Notched 1.07 - 2.14 J/cm
2.00 - 4.00 ft-lb/in
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester
BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in..
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Ashley Polymers Ashlene® 524 Nylon 66
A general purpose toughened Nylon 66.Data provided by the manufacturer
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced  (Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Izod Impact, Notched 1.07 J/cm

@Thickness 3.20 mm
2.00 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 385 TFE 15 SI 2 Polycarbonate (PC); Carbon Fiber - PTFE Lubricated - Silicone Lubricated
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Electrablend® PA6 CF20 BK 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Conductive, Heat Stabilized and Lubric..
Izod Impact, Notched 1.07 - 4.27 J/cm
2.00 - 8.00 ft-lb/in
ASTM D256
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Izod Impact, Notched 1.07 J/cm

@Thickness 3.17 mm
2.00 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 4605 Syndiotactic Polystyrene (SPS), Glass Fiber