Material Notes:
Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized. The main features of Grilamid L 25 W 10 HX are: Exceptional impact strength, also at low temperaturesHigh burst pressure resistanceLow density, low weightEasy processing Application examples: Grilamid L 25 W 10 HX is suitable for the production of semi-flexible tubes requiring good low temperature impact strength and burst pressure resistance for use in automotive (no direct gasoline/petrol contact) and industrial applications. This material is especially suited for use in high temperature Diesel lines.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Water Absorption 1.5 %
1.5 %
ISO 62
Moisture Absorption 0.700 %
0.700 %
ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
conditioned, 15s; ISO 868
Tensile Strength at Break 40.0 MPa
5800 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 35.0 MPa
5080 psi
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
>= 50 %
>= 50 %
dry; ISO 527-1/-2
Elongation at Yield 15 %
15 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.600 GPa
87.0 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 µm/m-°C
72.2 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 160 µm/m-°C
88.9 µin/in-°F
ISO 11359-1/-2
Melting Point 175 °C
347 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 120 °C
176 - 248 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Plasticizer
Automotive Compressed air systems
Fuel systems
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Product Attributes Flexible
High viscosity
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)