Polymer Property : Charpy Impact, Notched = 9.50 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® 104 PC
UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will..
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® 104R PC
UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant in limited colors.Effective January 15..
Charpy Impact, Notched 9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® IR2840 PC
7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant, natural only.Effective January 15th, 2007 this grade will no longer be supported with biocompatibilit..
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HP6 PC
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo..
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
ISO Data
Styron CALIBREâ„¢ 200 6 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
ISO Data
Styron CALIBREâ„¢ 300 6 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® R 50 H NZ PA6
Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V..
Charpy Impact, Notched 9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® FN714 NC010A Nylon 66
Zytel® FN714 NC010A is an impact modified, very flexible, plasticizer free polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
conditioned; ISO 179/1eA
EMS-Grivory Grivory® L 25 W 10 H X PA12
Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized..
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
BASF Novolen® 2900 H Polypropylene
Injection molded and thermoformed parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
ISO 179/1eA
BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry)
Ultramid B3ZG6 BK30564 is an impact-modified, pigmented black, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity.
Charpy Impact, Notched 9.50 J/cm²
45.2 ft-lb/in²
50%RH; Partial; ISO 179/1eA
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610  (Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient..