Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are marine applications and pump housings.
Physical Properties Metric English Comments
Specific Gravity 1.75 - 1.95 g/cc
1.75 - 1.95 g/cc
Water Absorption 0.10 - 0.15 %
0.10 - 0.15 %
24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 50
40 - 50
Tensile Strength, Ultimate 41.4 - 55.2 MPa
6000 - 8000 psi
Flexural Strength 96.5 - 138 MPa
14000 - 20000 psi
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Compressive Strength 124 - 138 MPa
18000 - 20000 psi
Izod Impact, Notched 2.14 - 5.34 J/cm
4.00 - 10.0 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 13.8 - 15.7 kV/mm
350 - 400 kV/in
Short Time
Arc Resistance >= 190 sec
>= 190 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F