Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 215 W1 902176 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, weather-stabilized |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 23.0 - 60.0 °C |
88.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY KX05015 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX05015 is a compound based on Acetal Copolymer resin containing Antistat. Added features include permanent Anti-Static. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 23.0 - 60.0 °C |
88.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA6.12 (Europe-Africa-Middle East) LNP THERMOCOMP* IF006 is a compound based on nylon 6/12 resin containing glass fibre |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 20.0 °C |
88.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Baydur® GS PIR A Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 20.0 °C |
88.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 20.0 °C |
88.9 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnitel® EM460 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BRZ 347 W PA6 Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 16 W 20 black 9995 PA12 Product Description: Grilamid L 16 W 20 is a semi-flexible low viscosity, heat stabilized PA12 injection molding grade. The main characteristics of this product are: Easy flowing?High impact streng.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20 W 20 grey 9280 PA12 Product Description: Grilamid L 20 W 20 grey 9280 is a semiflexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 grey 9280 is heat stabilized. The main featur.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20 W 20 PA12 Product Description: Grilamid L 20 W 20 is a semi-flexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 is heat stabilized. The main features of Grilamid L 20.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 3841 nat PA12 Product description: Grilamid XE 3841 is a flexible, heat stabilized and plasticizer-free Polyamide 12, which offers a very good processability for extrusion. Grilamid XE 3841 is qualified in Europe.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 3982 PA12 Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 23.0 - 60.0 °C |
88.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide P1000IX3 PA6, Impact Modified, Injection Molded Staramide P1000IX3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020 or Star X 2020)Information provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 W 20 PA12 Product Description: Grilamid L 25 W 20 is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 is UV and heat stabilized. The main features of Grila.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature 23.0 - 60.0 °C |
88.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermotuf P1000IX3 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* P1000IX3 is a compound based on PA6 resin containing Impact Modifier. Added features include : High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C @Temperature -30.0 - 100 °C |
88.9 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3230A PP SABIC® PPcompound G3230A is a general purpose, 30% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 109612410 |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | Average above Tg; ISO 11359 |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
CTE, linear, Transverse to Flow | 160 µm/m-°C | 88.9 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BR 40 W PA6 Product description: Grilon BR 40 W is a medium viscosity, plasticized PA6 extrusion grade. Grilon BR 40 W has the following important properties: High flexibilityHigh stiffness Grilon BR 40 W is us.. |