Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D638 |
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527-1/-2 |
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | |
Radici Radilon® S USZ200 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D638 |
3M Dyneon™ 1641 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D638 |
3M Dyneon™ 1645 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | Sintered Molding, DIN 53457 |
3M Dyneon™ 1502 PTFE Powder
(discontinued **) Type VI PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r.. |
|||
Tensile Modulus | 0.600 - 0.700 GPa | 87.0 - 102 ksi | DIN 53457 |
Isoflon PFA Polyperfluoroalkoxyethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Modulus | 0.600 - 0.700 GPa | 87.0 - 102 ksi | DIN 53457 |
Isoflon TFM Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 246M PA66, Conditioned Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BRZ 347 W PA6 Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Tensile Modulus | 0.600 GPa @Temperature 180 °C |
87.0 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TS300 PA46 |
|||
Tensile Modulus | 0.600 GPa @Temperature 180 °C |
87.0 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527-1/-2 |
DSM Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4181 black PA1010 Product description: Grilamid XE 4181 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 black 9992 is highly .. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | DIN 53 457 |
Hippe PE 1000 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527-1/-2 |
DSM Stanyl® TW363 Nylon 46 (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | MD |
BASF Ultramid® C40 LN 07 0.04 mm Blown Film Cold Air Information provided by BASF |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | Sintered Molding; ASTM D638 |
3M Dyneon™ TF 1750 PTFE Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very .. |
|||
Tensile Modulus | 0.600 GPa @Thickness 1.00 mm, Temperature 23.0 °C |
87.0 ksi @Thickness 0.0394 in, Temperature 73.4 °F |
1.0 mm/min; ASTM D1708 |
Solvay Specialty Polymers Hyflon® PFA P220 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Tensile Modulus | 0.600 GPa @Temperature 180 °C |
87.0 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TE300 PA46 Heat Stabilized |
|||
Tensile Modulus | >= 0.600 GPa | >= 87.0 ksi | DIN 53457 |
Adamas Adalon® 911 PTFE Information provided by Adamas, HPM |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | ISO 527-1/-2 |
Unitika EX-1030 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | 1mm/min; ISO 527-2 |
Borealis Borsoft™ SG220MO Polypropylene Random Copolymer for Injection Molding Borsoft™ SG220MO is a polypropylene characterized by good flow, high impact and good transparency. This grade contains antistatic and demolding additives which, together with enhanced nucleation, .. |
|||
Tensile Modulus | 0.600 GPa | 87.0 ksi | 1 mm/min |
Arkema Group Orgalloy® LT 6040 Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |