Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | |
Plastcom SLOVAMID 6 GF 50 TS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.016 cm/cm @Thickness 3.17 mm |
0.012 - 0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 7700 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.016 cm/cm @Thickness 3.17 mm |
0.012 - 0.016 in/in @Thickness 0.125 in |
ASTM D955 |
Network Polymers Softflex® 8910 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | 410°C nozzle, 220°C mold |
Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer
(discontinued **) Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in colorApplication Areas: Suitable for high temperature applica.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ASTM-D1204 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 25 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | 60x60x2; 250°C / WZ 70°C; 600 bar; ISO 294-4 |
Lanxess Pocan® DP C 1502 000000 PBT + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | |
LATI Latilub 57-30GRTS G/20 PPA, 20% Glass Fiber Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm @Time 86400 sec |
0.012 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp HF00ASU PA11 (Europe-Africa-Middle East) LNP* THERMOCOMP* HF00ASU is a compound based on PA11 resin containing Glass Fiber. Added features include; Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® F602G30 Nylon 66, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® N602G6S Nylon 66, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm @Thickness 2.00 mm |
0.012 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Proâ„¢ P701J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossHigh productivityGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfa.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | DIS 294-4 |
Wellman Wellamid® 42LN2-N Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | |
Toyobo Vylopet® EMC605 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: glossy surface componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanic.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 |
DSM Akulon® S223-G4U (Cond.) 23% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® HT3Z LF black 9564 PA* Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® L 25 W 20 Y PA12-I Product Description: Grilamid L 25 W 20 Y black 9992 is a semiflexible plasticized, medium viscosity, extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 Y black 9992 is impact modified, heat.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | Eurotec |
Eurotec® Tecomid® NB40 NL RM PA6, unfilled, MoS2, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® L 22A W 40 X PA12-I Product Description: Grilamid L 22A W 40 X is a flexible plasticized and impact modified heat and light stabilized Polyamide 12 (PA12). The main features of Grilamid L 22A W 40 X are: Good impact st.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | |
Eurotec® Tecodur® PB70 GR10 NL PBT 10% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | |
Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Conditioned, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.012 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® Rnew 70R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 70R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | Sheet |
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, .. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610