Material Notes:
Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy processingShort cycle times Grilon BS 23 is suitable for thin wall applications, where excellent flow behavior and short cycle times are a must.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Water Absorption 9.0 %
9.0 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 60.0 MPa
8700 psi
conditioned; ISO 2039-1
130 MPa
18900 psi
dry; ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
conditioned; ISO 527-1/-2
50.0 MPa
7250 psi
dry; ISO 527-1/-2
Tensile Strength, Yield 40.0 MPa
5800 psi
dry; ISO 527-1/-2
70.0 MPa
10200 psi
dry; ISO 527-1/-2
Elongation at Break 20 %
20 %
dry; ISO 527-1/-2
20 %
20 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
dry; ISO 527-1/-2
35 %
35 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.00 GPa
145 ksi
conditioned; ISO 527-1/-2
3.00 GPa
435 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
dry; ISO 179/1eU
10.0 J/cm²
47.6 ft-lb/in²
conditioned; ISO 179/1eU
4.50 J/cm²

@Temperature 30.0 °C
21.4 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
5.00 J/cm²

@Temperature 30.0 °C
23.8 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
dry; ISO 179/1eA
0.800 J/cm²
3.81 ft-lb/in²
conditioned; ISO 179/1eA
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
22.2 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
27.8 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 70.0 - 90.0 °C
158 - 194 °F
long term; EMS
140 °C
284 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 ohm-cm
1.00e+8 ohm-cm
dry; IEC 60093
1.00e+8 ohm-cm
1.00e+8 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+7 ohm
1.00e+7 ohm
IEC 60093
Dielectric Strength 5.00 kV/mm
127 kV/in
conditioned; IEC 60243-1
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Electricals & Electronics Electrical equipment
Form Granules
Industry & Consumer goods Mechanical Engineering
Power transmission
Tools & Accessories
Processing Injection Molding
Product Attributes Nucleated
Special Characteristics Anti-static
Copyright © lookpolymers.com All Rights Reserved