Polymer Property : Dielectric Strength = 5.00 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 5.00 kV/mm
127 kV/in
ASTM D149
Parker Chomerics THERM-A-GAP™ GEL T630 Dispensable, Very Low Compression Force, Thermal Gap Filler
Description: THERM-A-GAP™ Gels are highly conformable, pre-cured, single-component compounds. The cross-linked gel structure provides superior long therm thermal stability and reliable performance...
Dielectric Strength 5.00 kV/mm
127 kV/in
ASTM D149
Parker Chomerics THERM-A-GAP™ GEL T630G Dispensable, Very Low Compression Force, Thermal Gap Filler
Description: THERM-A-GAP™ Gels are highly conformable, pre-cured, single-component compounds. The cross-linked gel structure provides superior long therm thermal stability and reliable performance...
Dielectric Strength 5.00 kV/mm
127 kV/in
ASTM D149
Parker Chomerics THERM-A-GAP™ GEL T635 Dispensable, Very Low Compression Force, Thermal Gap Filler
Description: THERM-A-GAP™ Gels are highly conformable, pre-cured, single-component compounds. The cross-linked gel structure provides superior long therm thermal stability and reliable performance...
Dielectric Strength 5.00 kV/mm
127 kV/in
ASTM D149
Parker Chomerics THERM-A-GAP™ GEL T636 Dispensable, Very Low Compression Force, Thermal Gap Filler
Description: THERM-A-GAP™ Gels are highly conformable, pre-cured, single-component compounds. The cross-linked gel structure provides superior long therm thermal stability and reliable performance...
Dielectric Strength >= 5.00 kV/mm

@Thickness 1.00 mm
>= 127 kV/in

@Thickness 0.0394 in
in oil; ASTM D149
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific)
Thermally conductive mineral filled PPS FR compound
Dielectric Strength 5.00 kV/mm

@Thickness 1.00 mm
127 kV/in

@Thickness 0.0394 in
IEC 60243-P1
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application..
Dielectric Strength 5.00 - 45.0 kV/mm
127 - 1140 kV/in
Average value: 30.6 kV/mm Grade Count:18
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Dielectric Strength 5.00 kV/mm
127 kV/in
150°C for 1,000 hrs
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 5.00 kV/mm
127 kV/in
AC 60 Hz
Fujipoly Industries Sarcon® 20GSR Thin-Film GSR
Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of..
Dielectric Strength 5.00 kV/mm
127 kV/in
JIS-K-6249/ASTM D-149
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD
Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries
Dielectric Strength 5.00 kV/mm
127 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 45H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 5.00 kV/mm
127 kV/in
Shin-Etsu Silicones KE-3418 Silicone, RTV Adhesive
Information Provided by Shin-Etsu Silicones of America, Inc.
Dielectric Strength 5.00 kV/mm
127 kV/in
Shin-Etsu Silicones KE-3417 Silicone, RTV Adhesive
Information Provided by Shin-Etsu Silicones of America, Inc.
Dielectric Strength 5.00 kV/mm
127 kV/in
ASTM D149
Tipco Tipcolite® TG 311 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties
Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie..
Dielectric Strength 5.00 kV/mm
127 kV/in
ASTM D149
Tipco Tipcolite® TG 615 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties
Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie..
Dielectric Strength 5.00 kV/mm
127 kV/in
ASTM D149
Tipco Tipcolite® TMS 211 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength
Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr..
Dielectric Strength 5.00 kV/mm
127 kV/in
Dow Corning SE 4445 CV KIT
Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility, UL V-0.Information provided by Dow Corning
Dielectric Strength 5.00 kV/mm
127 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® BS EC PA6
Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy pro..
Dielectric Strength 5.00 kV/mm
127 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40
Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate..
Dielectric Strength 5.00 kV/mm
127 kV/in
Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antista..
Dielectric Strength 5.00 - 7.00 kV/mm

@Temperature 90.0 °C
127 - 178 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit..
Dielectric Strength 5.00 - 7.00 kV/mm

@Temperature 90.0 °C
127 - 178 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane..
Dielectric Strength 5.00 - 7.00 kV/mm

@Temperature 90.0 °C
127 - 178 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication ..
Dielectric Strength 5.00 - 44.5 kV/mm
127 - 1130 kV/in
Average value: 36.1 kV/mm Grade Count:18
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..
Dielectric Strength 5.00 kV/mm

@Thickness 1.00 mm
127 kV/in

@Thickness 0.0394 in
IEC 60243-P1
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed &n
Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-..
Dielectric Strength 5.00 kV/mm

@Thickness 1.00 mm
127 kV/in

@Thickness 0.0394 in
IEC 60243-P1
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed
Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou..