Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ASTM D638 |
Plaskolite Optix® Acrylic Sheet Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ASTM D638 |
Nylene® NX4301 Nylon 6, Extrusion Grade Dry as molded. Extrusion grade. Nylene NX4301 is a high viscosity, UV stabilized extrusion grade nylon resistant to degradation by ultraviolet light. The elevated quality of UV resistance is attri.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527-1,2 |
Qualchem Danamid FELX0 Polyamide 6 Flame retardant, halogen-free (V-0)Information provided by Qualchem Zrt. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 500RS PC (Europe-Africa-Middle East) LEXAN 500RS is a medium viscosity, glass reinforced, flame retardant grade. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 503RS PC (Europe-Africa-Middle East) LEXAN 503RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXM4701 PPC LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Americas .. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 70.0 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Tensile Strength, Yield | 70.0 - 93.1 MPa | 10200 - 13500 psi | Average value: 81.2 MPa Grade Count:4 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | ASTM D638 |
LG Chemical Lupox® PBT-GP-2306FA 30% GFR Flame Retardant, UV Stabilized PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 70.1 MPa @Thickness 3.20 mm |
10200 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 1-5820 20% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-5820 is a 20% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-5820 is recommended for producing in.. |
|||
Tensile Strength, Yield | 70.6 MPa | 10200 psi | ASTM D638 |
Samyang Trirex® 3030I Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific) Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. .. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ASTM D638 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527 |
Polyram PlusTek PA801 Nylon 6.6 Copolymer for Injection Molding, Impact Modified Impact modified Nylon 6.6 copolymer for injection molding application.Information provided by Polyram. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO R527 |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix HexPly® ES70 is a structural epoxy resin particularly well adapted to low pressure molding processes. This system is versatile and allows a polymerization from 100°C (212°F) up to 150°C (302°F).. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1606 is a 30% glass filled chemically coupled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 70.2 MPa | 10200 psi | ASTM D638M |
DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12120 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12120 have a cherry-red appearance which tur.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® SC655 NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC655 is a medium viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
Eurostar Staramide B28N PA6, Nucleated, Injection Molded Staramide B28N is a Nucleated and Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ASTM D638 |
Beijing Ranger Chem PBT 403 M-G10 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min |
Arkema Group Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,MHLR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good.. |
|||
Tensile Strength, Yield | 70.2 MPa | 10200 psi | ASTM D638 |
Cheng Yu Plastic A703G2 ABS 20% Glass Fiber Reinforced |
|||
Tensile Strength, Yield | 70.0 - 95.0 MPa | 10200 - 13800 psi | Average value: 83.1 MPa Grade Count:6 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | v = 50 mm/min; ISO 527-2 |
CENTROPLAST CENTROCARB Polycarbonate CENTROCARB is a transparent or semi-transparent plastic with high strength and impact resistance. It is dimensionally rigid and has very good electrical insulating properties. It is used in contain.. |