Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 TF20 Nylon 6.6 for injection molding, 20% PTFE lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Celanese Thermx® FG20GT NC010 PCT  (discontinued **)
Thermx® FG20GT NC010 is a 20% glass fiber reinforced, toughened modified polycyclohexylenedimethylene terephthalate resin suitable for repeated-use food-contact US FDA housewares applications.Celen..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO Data, Low Temp
Americas Styrenics Styron® 6010 High Impact Polystyrene  (discontinued **)
STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac..
Charpy Impact Unnotched 5.00 J/cm² - NB
23.8 ft-lb/in² - NB
Average value: 6.17 J/cm² Grade Count:13
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Charpy Impact Unnotched 5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 20-0659 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Charpy Impact Unnotched 5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Lanxess Pocan® B 3215 XF 000000 PBT, 10% Glass Fiber
PBT, 10% glass fibers, injection molding, improved flowability, impact modified
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1105/GR/15/TF/15-2 PEEK, with PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
LATI Lapex A G/10 PES, 10% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
LATI Latilub 66-15T G/30 PA66, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
Charpy Impact Unnotched 5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® 420SE0U PBT
PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized
Charpy Impact Unnotched 5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East)
VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin.
Charpy Impact Unnotched 5.00 J/cm²

@Temperature 30.0 °C
23.8 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® BG-30 FR PA6-GF30 FR
Information provided by EMS Grivory
Charpy Impact Unnotched 5.00 J/cm²

@Temperature 30.0 °C
23.8 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® EBGM-20 HX PA666-GF15
Product description: Grilon EBGM-20 HX black 9992 is a high viscosity, high heat stabilized PA66 + PA6 extrusion blow molding grade with 15% glass fibers. The special features of Grilon EBGM-20 HX b..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® GV-2H PA*-GF20
Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide...
Charpy Impact Unnotched 5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40
Product description: Grivory HTM-4H1 is a 40 % mineral reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA ..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40
Product description: Grivory HTM-4H1 is a 40 % mineral reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA ..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30
Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® HTV-3H1 nat PA6T/6I-GF30
Product description: Grivory HTV-3H1 natural is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30
Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following ..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Crastin® CE15330 BK010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® CE15330 BK010 is a 30% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
Edgew 80x10x4; ISO 179/1eU
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® GV-2 FWA black 9225 PA*-GF20
Product description: Grivory GV-2 FWA black 9225 is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copoly..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® HT1V-3 FWA nat PA6T/6I-GF30
Product description: Grivory HT1V-3 FWA natural is a 30 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6..
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
conditioned; ISO 179/1eU
EMS-Grivory Grivory® HT1V-3 FWA nat PA6T/6I-GF30
Product description: Grivory HT1V-3 FWA natural is a 30 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6..
Charpy Impact Unnotched 5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop..
Charpy Impact Unnotched 5.00 J/cm²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese Celstran® PP-GF40-0414 P10 PP, 40% Glass Reinforced
Material code according to ISO 1043-1: PPInformation provided by Celanese
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179
BASF Ultramid® B3GM35 Q611 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid B3GM35 Q611 is a 40% combined glass-fiber and mineral reinforced injection molding PA6 grade.
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179
Teijin Panlite® G-3415R Glass Fiber Reinforced Polycarbonate Resin
GF 15% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th..
Copyright © lookpolymers.com All Rights Reserved