Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 5.00 kV/mm | 127 kV/in | ASTM D149 |
Parker Chomerics THERM-A-GAP™ GEL T630 Dispensable, Very Low Compression Force, Thermal Gap Filler Description: THERM-A-GAP™ Gels are highly conformable, pre-cured, single-component compounds. The cross-linked gel structure provides superior long therm thermal stability and reliable performance... |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | ASTM D149 |
Parker Chomerics THERM-A-GAP™ GEL T630G Dispensable, Very Low Compression Force, Thermal Gap Filler Description: THERM-A-GAP™ Gels are highly conformable, pre-cured, single-component compounds. The cross-linked gel structure provides superior long therm thermal stability and reliable performance... |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | ASTM D149 |
Parker Chomerics THERM-A-GAP™ GEL T635 Dispensable, Very Low Compression Force, Thermal Gap Filler Description: THERM-A-GAP™ Gels are highly conformable, pre-cured, single-component compounds. The cross-linked gel structure provides superior long therm thermal stability and reliable performance... |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | ASTM D149 |
Parker Chomerics THERM-A-GAP™ GEL T636 Dispensable, Very Low Compression Force, Thermal Gap Filler Description: THERM-A-GAP™ Gels are highly conformable, pre-cured, single-component compounds. The cross-linked gel structure provides superior long therm thermal stability and reliable performance... |
|||
Dielectric Strength | >= 5.00 kV/mm @Thickness 1.00 mm |
>= 127 kV/in @Thickness 0.0394 in |
in oil; ASTM D149 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |
|||
Dielectric Strength | 5.00 kV/mm @Thickness 1.00 mm |
127 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, hot steam and hot water resistant (not suitable for use of higher voltage).Application.. |
|||
Dielectric Strength | 5.00 - 45.0 kV/mm | 127 - 1140 kV/in | Average value: 30.6 kV/mm Grade Count:18 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 20GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | JIS-K-6249/ASTM D-149 |
Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | 60°C for 500 hrs |
Fujipoly Industries Sarcon® 45H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | |
Shin-Etsu Silicones KE-3418 Silicone, RTV Adhesive Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | |
Shin-Etsu Silicones KE-3417 Silicone, RTV Adhesive Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | ASTM D149 |
Tipco Tipcolite® TG 311 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | ASTM D149 |
Tipco Tipcolite® TG 615 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | ASTM D149 |
Tipco Tipcolite® TMS 211 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | |
Dow Corning SE 4445 CV KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility, UL V-0.Information provided by Dow Corning |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BS EC PA6 Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy pro.. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40 Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Dielectric Strength | 5.00 kV/mm | 127 kV/in | |
Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antista.. |
|||
Dielectric Strength | 5.00 - 7.00 kV/mm @Temperature 90.0 °C |
127 - 178 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Dielectric Strength | 5.00 - 7.00 kV/mm @Temperature 90.0 °C |
127 - 178 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane.. |
|||
Dielectric Strength | 5.00 - 7.00 kV/mm @Temperature 90.0 °C |
127 - 178 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |
|||
Dielectric Strength | 5.00 - 44.5 kV/mm | 127 - 1130 kV/in | Average value: 36.1 kV/mm Grade Count:18 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Dielectric Strength | 5.00 kV/mm @Thickness 1.00 mm |
127 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed
&n Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-.. |
|||
Dielectric Strength | 5.00 kV/mm @Thickness 1.00 mm |
127 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou.. |