Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Hytrel® 4053FG TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer DuPont Performance Polymers
Trade Name Hytrel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® 4053FG TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hytrel® 4053FG is a low modulus high performance thermoplastic elastomer with food compliance specificity. It is suitable for extrusion and injection molding processes.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.159 g/cc
0.04187 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.00020 cm/cm
0.00020 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0037 cm/cm
0.0037 in/in
ISO 294-4
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 38

@Temperature 23.0 °C,
Time 15.0 sec
38

@Temperature 73.4 °F,
Time 0.00417 hour
ISO 868
44

@Temperature 23.0 °C,
Time 1.00 sec
44

@Temperature 73.4 °F,
Time 0.000278 hour
ISO 868
Tensile Strength at Break 26.0 MPa

@Temperature 23.0 °C
3770 psi

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Stress 2.40 MPa

@Strain 5.00 %,
Temperature 23.0 °C
348 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
4.10 MPa

@Strain 10.0 %,
Temperature 23.0 °C
595 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
7.30 MPa

@Strain 50.0 %,
Temperature 23.0 °C
1060 psi

@Strain 50.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
Elongation at Break 470 %

@Temperature 23.0 °C
470 %

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Modulus 0.0560 GPa

@Temperature 23.0 °C
8.12 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 9.90 J/cm²

@Temperature -30.0 °C
47.1 ft-lb/in²

@Temperature -22.0 °F
partial break; ISO 179/1eA
13.7 J/cm²

@Temperature -40.0 °C
65.2 ft-lb/in²

@Temperature -40.0 °F
partial break; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 155 °C
311 °F
10°C/min; ISO 11357-1/-3
Processing Properties Metric English Comments
Melt Temperature 180 °C
356 °F
Optimum; Extrusion
180 °C
356 °F
Optimum; Injection Molding
Mold Temperature 30.0 - 40.0 °C
86.0 - 104 °F
Injection Molding
Drying Temperature 80.0 °C
176 °F
Extrusion
80.0 °C
176 °F
Injection Molding
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Extrusion
3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding
Moisture Content <= 0.080 %
<= 0.080 %
Extrusion
<= 0.080 %
<= 0.080 %
Injection Molding
Descriptive Properties Value Comments
Appearance Natural Color
Forms Pellets
Generic TPC-ET
Material Status Current
Part Marking Code >TPC-ET<
ISO 11469
Processing Method Injection Molding
Product Category Extrusion Resins
Food Contact Resins
High Performance Hytrel®® Resins
Unreinforced Resins
Region Available - Global Yes
Resin Identification TPC-ET
ISO 1043
RoHS Compliance Contact Manufacturer
Uses Food Applications, Non-specific