Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Plastcom SLOVALEN PH 71 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Melting Point | 155 - 161 °C | 311 - 322 °F | |
Oceanchem Group Antioxidant 1098 Molecular Formula: C40H64O4N4Cas No.: 23128-74-7Use: This product is a non-color-degrading, nonpolluting, heat-resisting, extraction-resisting, high-performance all-purpose antioxidant, mainly appli.. |
|||
Melting Point | 155 - 170 °C | 311 - 338 °F | ASTM D3418 |
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co.. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1.. |
|||
Melting Point | 155 - 160 °C | 311 - 320 °F | |
Hong Kun Group AO 1098 Antioxidant Chemical Name: 3,3'-Bis(3,5-di-tert-butyl-4-hydroxyphenyl)-N,N'-hexamethylenedipropionamideCAS No. 23128-74-7All information provided by Hongkun Group |
|||
Melting Point | 155 - 173 °C | 311 - 343 °F | Huntsman/TMA |
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Melting Point | >= 155 °C | >= 311 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | >= 155 °C | >= 311 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® F 1130 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | 155 °C | 311 °F | DIN EN ISO 314 |
GEHR Plastics PA 12 TR Transparent Nylon 12 Used for optical components that benefit from the transparency and the high dynamic strengthProperties:TransparencyExtremely high dynamic strengthHigh chemical resistanceHigh stress-cracking resista.. |
|||
Melting Point | 155 °C | 311 °F | TMA; MCI Method |
Mitsui APELâ„¢ APL6015T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Melting Point | 155 °C | 311 °F | ASTM D2117 |
Lushan PR296B Adhesive Resin for Aluminum Plastic Composite Pipe Adhesive resin Lushan series for aluminum-plastic composite pipe is maleic grafted polyethylene used for PE-AL-PE, PEX-AL-PEX and PERT-AL-PERT composite pipes. Lushan adhesive resin could provides i.. |
|||
Melting Point | 155 - 175 °C | 311 - 347 °F | Huntsman/TMA |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
Melting Point | <= 155 °C | <= 311 °F | |
Struktol CALCIUM STEARATE GR High purity, non-wettable, calcium stearate granule.STRUKTOL® Calcium Stearate GR is an effective processing aid and release agent. The low chloride content of STRUKTOL® Calcium Stearate GR al.. |
|||
Melting Point | 155 °C | 311 °F | Kofler |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |
|||
Melting Point | 155 - 159 °C | 311 - 318 °F | ISO 3146 |
Borealis Daploy™ SF203HMS High Melt Strength Polypropylene for Extrusion Coating Daploy SF203HMS resin is a statistic-heterophasic-propylene-ethylene copolymer modified with a polypropylene based structurally isomeric polymer which combines a significantly increased melt strengt.. |
|||
Melting Point | 155 °C | 311 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® 30HS Polyester Elastomer TPC-ET
(Unverified Data**) Polyester Elastomer Concentrate Developed for Enhancing Heat Ageing ResistanceInformation provided by DuPont Performance Polymers |
|||
Melting Point | 155 °C | 311 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® 4053FG TPC-ET
(Unverified Data**) Hytrel® 4053FG is a low modulus high performance thermoplastic elastomer with food compliance specificity. It is suitable for extrusion and injection molding processes.Information provided by DuPon.. |
|||
Melting Point | 155 - 160 °C | 311 - 320 °F | |
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Melting Point | 155 - 160 °C | 311 - 320 °F | |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Melting Point | 155 - 160 °C | 311 - 320 °F | |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Arkema Group KYNAR® 461 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |
|||
Melting Point | 155 °C | 311 °F | ISO 3146 |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Arkema Group KYNAR® 301-F Polyvinylidene Fluoride Powder Characteristics: Fine milled, white, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abra.. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Melting Point | 155 - 160 °C | 311 - 320 °F | |
Arkema Group KYNAR® Latex 32 Polyvinylidene Fluoride Water base, fine particle sizeInformation provided by Arkema Inc. |
|||
Melting Point | 155 - 160 °C | 311 - 320 °F | |
Arkema Group KYNAR FLEX® 2850 PC Polyvinylidene Fluoride Spray Coating Powder Electrostatic sprayInformation provided by Arkema Inc. |
|||
Melting Point | 155 - 160 °C | 311 - 320 °F | |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Melting Point | 155 - 165 °C | 311 - 329 °F | |
Arkema Group KYNAR® 201 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan.. |