Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 5.3 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 5.3 g/10 min
5.3 g/10 min
(Condition L) ASTM D-1238
Multibase Multi-Flex® TPE D 4308 BLK
The moisture content is 0.04%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin  (discontinued **)
Features: Octene co-polymer, excellent sealability and toughness, high drawdown, high adhesion, good barrier, good abrasion resistance.Applications: Food packaging, milk cartons, paperboard containe..
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 250 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Melt Flow 5.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
old Condition G; ASTM D1238
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer
Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli..
Melt Flow 5.3 - 10.3 g/10 min

@Load 1.20 kg,
Temperature 250 °C
5.3 - 10.3 g/10 min

@Load 2.65 lb,
Temperature 482 °F
Kazanorgsintez PC-075DA Polycarbonate
Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well ..
Melt Flow 5.3 g/10 min

@Load 6.60 kg,
Temperature 337 °C
5.3 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM 2300R PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Melt Flow 5.3 g/10 min

@Load 6.60 kg,
Temperature 337 °C
5.3 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM 2300R PEI (Asia Pacific)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Melt Flow 5.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Melt Flow 5.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Melt Flow 5.3 g/10 min

@Load 5.00 kg,
Temperature 280 °C
5.3 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL PN275 PPE+PS
PPE+PS with low mineral loading. High heat, platable applications.
Melt Flow 5.3 g/10 min

@Load 5.00 kg,
Temperature 280 °C
5.3 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL PN275F PPE+PS
PPE+PS with low mineral loading. High heat, platable applications. NSF approved for water contact applications.
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Total PPH 5069 Polypropylene Homopolymer, Fiber
Polypropylene PPH 5069 is a homopolymer polypropylene with a Melt Flow index of 6 g/10 min.Polypropylene PPH 5069 is intended for extrusion of high tenacity staple fibers for non-woven applications...
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Hytrel® 4053FG TPC-ET  (Unverified Data**)
Hytrel® 4053FG is a low modulus high performance thermoplastic elastomer with food compliance specificity. It is suitable for extrusion and injection molding processes.Information provided by DuPon..
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 235 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Conditioned)
Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to ..
Melt Flow 5.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin
STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™..
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 235 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Dry)
Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to ..
Melt Flow 5.3 g/10 min

@Load 2.16 kg,
Temperature 235 °C
5.3 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Arkema Group Cristamid® MS 1100 Semi-Aromatic Nylon (PASA) (Dry)
Designation ISO 1874-PA12/xx,MHLR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good..
Copyright © lookpolymers.com All Rights Reserved