Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 4.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 4.10 MPa

@Strain 100 %
595 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3880H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 4.10 MPa

@Strain 100 %
595 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® XG5858 TPC-ET
Injection Molding
Tensile Stress 4.10 MPa

@Strain 2.28 %,
Temperature 150 °C
595 psi

@Strain 2.28 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 4.10 MPa

@Strain 2.28 %,
Temperature 150 °C
595 psi

@Strain 2.28 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for ..
Tensile Stress 4.10 MPa

@Strain 10.0 %
595 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 4.10 MPa

@Strain 10.0 %,
Temperature 23.0 °C
595 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® 4053FG TPC-ET  (Unverified Data**)
Hytrel® 4053FG is a low modulus high performance thermoplastic elastomer with food compliance specificity. It is suitable for extrusion and injection molding processes.Information provided by DuPon..
Tensile Stress 4.10 MPa

@Strain 100.63 %,
Temperature 100 °C
595 psi

@Strain 100.63 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 4.10 MPa

@Strain 0.0400 %,
Temperature -40.0 °C
595 psi

@Strain 0.0400 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te..
Tensile Stress 4.10 MPa

@Strain 50.0 %
595 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers