Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company PCAB250 Acrylonitrile Butadiene Styrene + PC

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer M. Holland Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company PCAB250 Acrylonitrile Butadiene Styrene + PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High heat resistanceHigh impact resistanceLow temperature impact resistanceApplications: Automotive
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
23/23°C; ASTM D792
Melt Flow 4.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
73°F; ASTM D256
4.81 J/cm

@Temperature -28.9 °C
9.00 ft-lb/in

@Temperature -20.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Forms Pellets
Processing Methods Injection molding