Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carmel Olefins CAPILENE® HU 75 AV Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® HU 75 AV Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAPILENE® HU 75 AV is a nucleated and antistatic controlled rheology impact copolymer for injection molding. It is characterized by improved stiffness and medium impact resistance. CAPILENE® HU 75 AV has been formulated to allow short cycle time.Applications: CAPILENE® HU 75 AV has been especially developed for injection molding of pails and containers. This grade is also used for the injection molding of furniture, toys, housewares and technical items.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 33 g/10 min

@Load 2.16 kg,
Temperature 230 °C
33 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
50 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 0.350 J/cm

@Temperature -20.0 °C
0.656 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.650 J/cm

@Temperature 23.0 °C
1.22 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Vicat Softening Point 147 °C

@Load 1.02 kg
297 °F

@Load 2.25 lb
ASTM D1525