Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.40 MPa @Strain 100 % |
348 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S EF 70A-3S1975 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Tensile Stress | 2.40 MPa @Strain 100 % |
348 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S EH 70A-3S7004 Thermoplastic Elastomer (TPE) OnFlex™-S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tensile Stress | 2.40 MPa @Strain 100 % |
348 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S KA 60A-3S1769 Thermoplastic Elastomer (TPE) OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Stress | 2.40 MPa @Strain 100 % |
348 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® F7860 TPE, Fire Retardant Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome.. |
|||
Tensile Stress | 2.40 MPa @Strain 300 % |
348 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P2850 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.40 MPa @Strain 5.00 %, Temperature 23.0 °C |
348 psi @Strain 5.00 %, Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |
|||
Tensile Stress | 2.40 MPa @Strain 300 % |
348 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1750 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.40 MPa @Strain 5.00 % |
348 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 5.00 %, Temperature 23.0 °C |
348 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® 4053FG TPC-ET
(Unverified Data**) Hytrel® 4053FG is a low modulus high performance thermoplastic elastomer with food compliance specificity. It is suitable for extrusion and injection molding processes.Information provided by DuPon.. |
|||
Tensile Stress | 2.40 MPa @Strain 5.00 % |
348 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 103.36 %, Temperature 120 °C |
348 psi @Strain 103.36 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 5.00 % |
348 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 5.00 % |
348 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 5.00 % |
348 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 124.88 %, Temperature 200 °C |
348 psi @Strain 124.88 %, Temperature 392 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 0.360 %, Time 3.60e+7 sec |
348 psi @Strain 0.360 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 2.40 MPa @Strain 0.201 %, Time 3600 sec |
348 psi @Strain 0.201 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 2.40 MPa @Strain 0.287 %, Time 360000 sec |
348 psi @Strain 0.287 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 2.40 MPa @Strain 0.324 %, Time 3.60e+6 sec |
348 psi @Strain 0.324 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 2.40 MPa @Strain 0.244 %, Time 36000 sec |
348 psi @Strain 0.244 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |
|||
Tensile Stress | 2.40 MPa @Strain 0.444 %, Time 3.60e+6 sec |
348 psi @Strain 0.444 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 0.558 %, Time 3.60e+7 sec |
348 psi @Strain 0.558 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 0.261 %, Time 36000 sec |
348 psi @Strain 0.261 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 0.340 %, Time 360000 sec |
348 psi @Strain 0.340 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.40 MPa @Strain 0.202 %, Time 3600 sec |
348 psi @Strain 0.202 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |