DuPont Performance Polymers Crastin® SK612SF BK591 PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® SK612SF BK591 PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crastin® SK612SF BK591 is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production. It is laser markable.Information provided by DuPont
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Filler Content 15 %
15 %
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa

@Temperature 23.0 °C
16000 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break 3.3 %

@Temperature 23.0 °C
3.3 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 5.90 GPa

@Temperature 23.0 °C
856 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact Unnotched 2.70 J/cm²

@Temperature 23.0 °C
12.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 224 °C
435 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 201 °C
394 °F
ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 240 °C
464 °F
Optimum; Injection Molding
235 - 260 °C
455 - 500 °F
Injection Molding
Mold Temperature 80.0 °C
176 °F
Optimum; Injection Molding
30.0 - 130 °C
86.0 - 266 °F
Injection Molding
Drying Temperature 110 - 130 °C
230 - 266 °F
Injection Molding
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dehumidified Dryer; Injection Molding
Moisture Content <= 0.040 %
<= 0.040 %
Injection Molding
Descriptive Properties Value Comments
Appearance Black Color
Drying Recommended Yes
Injection Molding
Features Flow, High
Laser markable
Molding Cycle, Fast
Viscosity, Low
Filler Glass fiber
Generic PBT
Material Status Preliminary Data
Part Marking Code >PBT-GF15<
ISO 11469
Processing Method Injection Molding
Product Category Glass Reinforced Resins
Region Available - Americas Yes
Region Available - Asia/Pacific Yes
Region Available - Europe Yes
Resin Identification PBT-GF15
ISO 1043
RoHS Compliance Contact Manufacturer