Polymer Property : Melt Temperature = 455 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese Celanex® 1700FC PBT  (Unverified Data**)
Celanex 1700FC is a very high molecular weight extrusion grade of unreinforced polybutylene terephthalate for use in food contact applications.high molecular weight, unfilled PBT for use in food con..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese Celanex® 2401 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese Celanex® 3400-2 PBT, 40% Glass Reinforced  (Unverified Data**)
Celanex 3400-2 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese Celanex® 4022 PBT, Specialty  (Unverified Data**)
A white PBT resin typically used for applications requiring very opaque parts.PBT, opaque whiteInformation provided by Celanese
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese Celanex® 4302 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.30% glass-fiber, impact modifiedInformation provided by Celanese
Melt Temperature 235 °C
455 °F
Polyplastic Armlen® PP MF 25-3-901 Polypropylene, 20% Mineral Filled
Heat stabilized, black colorInformation provided by PolyPlastic Group.
Melt Temperature 235 - 260 °C
455 - 500 °F
Start Point: 240°C
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
Melt Temperature 235 - 245 °C
455 - 473 °F
Injection Molding
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant
Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b..
Melt Temperature 235 - 249 °C
455 - 480 °F
LG Chemical Lupox® PBT-GP-1000 High Flow PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Melt Temperature 235 - 265 °C
455 - 509 °F
Injection Molding
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid..
Melt Temperature 235 - 260 °C
455 - 500 °F
ISO 294
Gromax BPR20-N1 Nylon 6, Flame Retardant (Dry)
Information provided by Gromax Enterprises Corp.
Melt Temperature 235 - 265 °C
455 - 509 °F
Injection Molding
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Melt Temperature 235 - 285 °C
455 - 545 °F
Extrusion Coating
DuPont™ Appeel® 20D855 Ethylene Acrylate
DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
Melt Temperature <= 235 °C
<= 455 °F
CoExtrusion with EVA Processing
DuPont™ Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melt Temperature 235 - 305 °C
455 - 581 °F
Extrusion Coating
DuPont™ Nucrel® 3990L Ethylene Acrylic Acid
Nucrel® 3990L is a copolymer of ethylene and acrylic acid. It is available for use in conventional extrusion coating, coextrusion coating and extrusion laminating equipment. 9.5 % By Weight Acrylic..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese CELANEX 1602Z PBT, Unfilled
Celanex 1602Z is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1602Z has an internal lubricant.Information provi..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese CELANEX 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese CELANEX 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese
Melt Temperature 235 - 255 °C
455 - 491 °F
Celanese CELANEX 3216HR PBT, 15% Glass Reinforced
Celanex 3216HR is a flame retarded, hydrolysis resistant, 15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability.Information ..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese CELANEX 3425HRT PBT, Glass Reinforced
Celanex 3425HRT is a non-lubricated, 40% fiberglass reinforced PBT copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at break.Information provided..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese Celanex® 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese Cor..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese Celanex® 3226 PBT, Glass Reinforced
Celanex 3226 is a non-exuding, 20% glass-filled, flame retarded polybutylene terephthalate (PBT) which has an excellent balance of mechanical properties and processability. It is well suited for ele..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese Celanex® 602AC PBT, Glass Reinforced
Celanex 602AC is a 10% fiberglass reinforced PBT that has lower warpage and improved impact over standard PBT.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a ..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese CELANEX 3300-2LM PBT, Glass Reinforced
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release. It is a lasermarkable grade available i..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese CELANEX 531HS PBT, Glass Reinforced
Celanex 531HS is a 30% fiberglass reinforced PBT which has an excellent balance of mechanical properties and processability. Celanex 531HS is specifically designed to exhibit excellent thermal shoc..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese Celanex® 2002UV PBT, Unfilled
Celanex 2002UV is a general purpose,unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability and UV resistance. Celanex 2002UV is a medium flow materialTo..
Melt Temperature 235 - 260 °C
455 - 500 °F
Celanese RITEFLEX 677 TPC, Unfilled
Riteflex 677 is a thermoplastic polyester elastomer with nominal hardness of 77 shore D and high modulus.Information provided by Celanese
Melt Temperature 235 - 260 °C
455 - 500 °F
Start Point: 250°C
Kingfa JE2-R2G30 Glass Fiber Reinforced ABS/PBT Alloy
Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a..
Melt Temperature 235 - 250 °C
455 - 482 °F
Extrusion
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET  (Unverified Data**)
Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont
Melt Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET  (Unverified Data**)
Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont