Processing Properties Metric English Comments
Drying Temperature 110 - 130 °C
230 - 266 °F
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT  (Unverified Data**)
Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta..
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese Celanex® 2001FC PBT  (Unverified Data**)
Celanex 2001FC is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications for use in food contact applications...
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese Celanex® 4300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300LM is a toughened 30% glass reinforced PBT that is enhanced for improved laser marking graphics.30% glass fiber, good impact strength, laser markableInformation provided by Celanese
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese Celanex® 4306 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4306 is a 30% glass reinforced, toughened, low warpage thermoplastic polyester.30% glass-fiber, impact modified, low warpInformation provided by Celanese
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese Celanex® 6400-2 PBT, Mineral / Glass Reinforced  (Unverified Data**)
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.40% glass/mineral filled, low warpInformation provided by Celanese
Drying Temperature 110 - 130 °C

@Time 10800 sec
230 - 266 °F

@Time 3.00 hour
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Drying Temperature 120 - 130 °C

@Time 10800 sec
248 - 266 °F

@Time 3.00 hour
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Drying Temperature 110 - 130 °C

@Time 10800 sec
230 - 266 °F

@Time 3.00 hour
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Drying Temperature 110 - 130 °C

@Time 10800 sec
230 - 266 °F

@Time 3.00 hour
LATI Later 4 G/30-V0CT2 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Drying Temperature 120 - 130 °C

@Time 10800 sec
248 - 266 °F

@Time 3.00 hour
LATI Latigray 75/4-01 CX/45 PBT
Radiopaque compound based on Polybutylene Terephthalate (PBT). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by L..
Drying Temperature 120 - 130 °C

@Time 10800 sec
248 - 266 °F

@Time 3.00 hour
LATI Latilon 28D-V0 PC, Flame Retardant
Polycarbonate (PC) based compound. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. Very high dimensional stability. Ve..
Drying Temperature 110 - 130 °C
230 - 266 °F
LATI Latishield 87/28-10A G/20 PC, Steel/Glass Fiber Reinforced
EMI shielding product based on Polycarbonate (PC). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Drying Temperature 110 - 130 °C
230 - 266 °F
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A..
Drying Temperature 110 - 130 °C
230 - 266 °F
Samyang Tribit® 1503S Polybutylene Terephthalate
Characteristics:High impactApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samyang
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese CELANEX 2001FC PBT, Unfilled
Celanex 2001FC is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications for use in food contact applications...
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese CELANEX 2003HR PBT, Unfilled
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese CELANEX 2004-2 PBT, Unfilled
Celanex 2004-2 is an unfilled polyester that has an excellent combination of flowability and toughness. A typical application for Celanex 2004-2 is electrical connectors containing latches. Celanex ..
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese CELANEX 3316HR PBT, 30% Glass Reinforced
Celanex 3316HR is a flame retarded, hydrolysis resistant, 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability.Information..
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese Celanex® 3226 PBT, Glass Reinforced
Celanex 3226 is a non-exuding, 20% glass-filled, flame retarded polybutylene terephthalate (PBT) which has an excellent balance of mechanical properties and processability. It is well suited for ele..
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese Celanex® 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityTo avoid hydrolytic degradation during processi..
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese Celanex® 6407HR PBT, 30% Mineral / Glass Reinforced
Celanex 6407HR is a 30% glass/mineral reinforced hydrolysis resistant polyester particularly suited for large exterior automotive components where extended flow, flatness, and good surface appearanc..
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese VANDAR 6000 PBT, Unfilled
Vandar 6000 is a toughened polyester alloy with excellent cold temperature impact resistance.Information provided by Celanese
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese CELANEX 6400-2 PBT, Mineral / Glass Reinforced
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.Information provided by Celanese
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese CELANEX 7716 PBT, 35% Mineral / Glass Reinforced
Celanex 7716 is a 35% glass/mineral reinforced, non exuding, flame retarded polybutylene terephthlate which has and excellent balance of mechanical properties and processability. Celanex 7716 is wel..
Drying Temperature 110 - 130 °C
230 - 266 °F
DuPont Performance Polymers Crastin® HR5330HF BK503 PBT  (Unverified Data**)
Crastin® HR5330HF is a 30% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese Celanex® 1400FC PBT  (Unverified Data**)
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese Celanex® 6407 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.30% glass/mi..
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese Vandar® 2100UV PBT, Impact Modified  (Unverified Data**)
Vandar 2100UV is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional sta..
Drying Temperature 116 - 130 °C
240 - 266 °F
Average value: 123 °C Grade Count:8
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..
Drying Temperature 120 - 130 °C
248 - 266 °F
Celanese CELANEX 4302 PBT, 30% Glass Reinforced
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.Information provided by Celanese