Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Clariant Renol PPSSP0008 Polyphenylene Sulfide, Carbon Fiber, Lubricated

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PPSSP0008 Polyphenylene Sulfide, Carbon Fiber, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Mechanical Properties Metric English Comments
Tensile Strength, Yield 165 MPa
24000 psi
ASTM D638
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Temperature 22.8 °C
1.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 266 - 268 °C
510 - 515 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity <= 1e+05
<= 1e+05
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 307 - 329 °C
585 - 625 °F
Mold Temperature 135 - 177 °C
275 - 350 °F
Dry Time 2 - 4 hour

@Temperature 93.3 °C
2 - 4 hour

@Temperature 200 °F
to ensure moisture content level is less than 0.2%
Injection Pressure 41.4 - 74.5 MPa
6000 - 10800 psi
Secondary
68.9 - 103 MPa
10000 - 15000 psi
Initial
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 60 - 100 rpm
60 - 100 rpm