Mechanical Properties Metric English Comments
Flexural Modulus 20.7 GPa
3000 ksi
1.3 mm/min; ASTM D790
PolyOne LubriOne™ SF-30CF/15T Polyphenylene Sulfide (PPS)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Modulus 20.7 GPa

@Temperature 23.9 °C
3000 ksi

@Temperature 75.0 °F
Dry; 325°F 2kpsi; ASTM D790
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Chopped Molding Compound Reinforced
Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz..
Flexural Modulus 20.7 GPa

@Temperature 23.9 °C
3000 ksi

@Temperature 75.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 7781 E-Glass Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
PolyOne Edgetek® NN-40CF/000 - OBSOLETE Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 3483-3 Liquid Crystal Polymer (LCP), Carbon Fiber
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
PolyOne Edgetek® PS-30CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 4011 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 4011 Polyphthalamide (PPA), Glass Fiber
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
PolyOne Edgetek® PK-40CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 4085 A TFE 15 (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - PTFE Lubricated
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 4099 X 131005 B Polyphthalamide (PPA), Thermally Conductive - Electrically Conductive
Preliminary Data Sheet
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 4285 TFE 15 Thermoplastic Polyimide (TPI), Carbon Fiber - PTFE Lubricated
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
RTP Company RTP 3885 Polyaryletherketone (PAEK), Carbon Fiber 30%  (discontinued **)
Data is for injection molded specimens and was provided by the manufacturer, RTP Company.This product has been discontinued, please contact RTP Company regarding alternate grades.
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 4485 TFE 15 High Temperature Nylon (HTN), Carbon Fiber - PTFE Lubricated
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 4785 FR Polytrimethylene Terephthalate (PTT), Carbon Fiber - Flame Retardant
Flexural Modulus 20.7 GPa
3000 ksi
Lengthwise; ASTM D790
G-11 Fiberglass Epoxy Laminate Sheet
This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e..
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
PolyOne Edgetek® SF-30CF/000 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
PolyOne Lubri-Tech™ SF-30CF/13T2S Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE/Silicone Lubricated &n
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
RTP Company RTP 287D  Nylon 6/12 (PA 6/12) Carbon Fiber 40%  (discontinued **)
Carbon Fiber 40%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
RTP Company RTP 285D TFE 10  Nylon 6/12 (PA 6/12) Carbon Fiber 30% - PTFE 10%  (discontinued
Carbon Fiber 30% - PTFE 10%Comments:Carbon FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provi..
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
Techmer ES HiFill® PA6 CF40 40% Carbon Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAppearance: Black and Natural ColorInformation provided by TP Composites, Inc.
Flexural Modulus 20.7 GPa
3000 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED
LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
Flexural Modulus 20.7 GPa

@Temperature 23.0 °C
3000 ksi

@Temperature 73.4 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric
Information provided by HexCel
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 1485 Polyethersulfone (PES), Carbon Fiber
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 1385 C AR 10 TFE 15 Polyphenylene Sulfide (PPS), Carbon & Aramid Fiber Reinforced - PTFE Lubricated
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 200 TC-C-20 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Conductive - Flame Retardant
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790
RTP Company RTP 200 TC-C-40 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Conductive - Flame Retardant
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D790
RTP Company RTP 4285 TFE 5  Thermoplastic Polyimide (TPI) Carbon Fiber 30% - PTFE 5%  (disco
Carbon Fiber 30% - PTFE 5%Comments:Carbon FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provid..
Flexural Modulus 20.7 GPa
3000 ksi
ASTM D 790