Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 510 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® SF-40GF-10 MN/000 Polyphenylene Sulfide (PPS), Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 510 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® SF-47GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 510 °F | ASTM D648 |
Techmer ES Electrafil® J-1305/CF/30/TF/15 BK PPS |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 510 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PPS 0231 B LE Availability: North AmericaForms: PelletsFeatures: High Density and Low ExtractablesAppearance: OpaqueInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 510 °F | ASTM D648 |
Techmer ES Plaslube® J-1305/CF/15/TF/15 NAT PPS |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 510 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PPS 0237 A Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 510 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® SF-45GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 266 °C | 510 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® AM-30GM/15TF Polyphthalamide (PPA), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |