Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.8 - 15.7 kV/mm | 300 - 400 kV/in | ASTM D149 |
Ensinger Tecamid® 6/6 Nylon (PA66) Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)Information provided by Ensinger, Inc. |
|||
Dielectric Strength | 11.8 - 15.7 kV/mm @Thickness 3.17 mm |
300 - 400 kV/in @Thickness 0.125 in |
Short time value |
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
Dielectric Strength | 15.0 - 15.7 kV/mm | 380 - 400 kV/in | Short Time |
Bulk Molding Compounds BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impa.. |
|||
Dielectric Strength | 13.8 - 15.7 kV/mm | 350 - 400 kV/in | Short Time |
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,.. |
|||
Dielectric Strength | 14.6 - 15.7 kV/mm | 370 - 400 kV/in | short time |
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Dielectric Strength | 13.8 - 15.7 kV/mm | 350 - 400 kV/in | short time |
Bulk Molding Compounds BMC T9 General Purpose Molding Compound BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9.. |
|||
Dielectric Strength | 11.8 - 15.7 kV/mm | 300 - 400 kV/in | |
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Dielectric Strength | 11.8 - 15.7 kV/mm | 300 - 400 kV/in | |
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Dielectric Strength | 11.8 - 15.7 kV/mm | 300 - 400 kV/in | |
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Dielectric Strength | 13.8 - 15.7 kV/mm | 350 - 400 kV/in | Short Time |
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings. |
|||
Dielectric Strength | 14.6 - 15.7 kV/mm | 370 - 400 kV/in | Short Time |
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re.. |
|||
Dielectric Strength | 13.8 - 15.7 kV/mm | 350 - 400 kV/in | Short Time |
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an.. |
|||
Dielectric Strength | 14.6 - 15.7 kV/mm | 370 - 400 kV/in | short time |
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty.. |
|||
Dielectric Strength | 3.94 - 15.7 kV/mm | 100 - 400 kV/in | Average value: 13.1 kV/mm Grade Count:6 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Dielectric Strength | 13.8 - 15.7 kV/mm | 350 - 400 kV/in | short time |
Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression.. |
|||
Dielectric Strength | 13.8 - 15.7 kV/mm | 350 - 400 kV/in | short time |
Bulk Molding Compounds BMC T15(GPT) General Purpose Molding Compound BMC T15(GPT) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPT) is well suited for injection, transfer or compression.. |
|||
Dielectric Strength | 13.8 - 15.7 kV/mm | 350 - 400 kV/in | short time |
Bulk Molding Compounds BMC T45HT Automotive Grade Molding compound BMC T45HT was designed for the very demanding applications of automotive under hood engine covers. It meets the GMP UP .007 specification for automotive under hood. BMC T45HT is a vinyl ester base.. |