Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 190 - 195 sec | 190 - 195 sec | ASTM D495 |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Cookson Group Plaskon® 435 Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Combines exceptional reliability with wide molding process latitude. This material is designed to encapsulate a variety of semic.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Haysite 20000 Polyester BMC, 15% Glass Reinforced The 20000 series bulk molding compound is an electrical grade that can be compression, transfer, or injection molded. Offering good arc/track properties and mechanical strength, this grade is also r.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Haysite H900 Polyester, Glass Reinforced H900 is recognized throughout the world as a reliable, consistent GPO-3 material. Standard size sheets are available in thicknesses ranging from .094" to 2.00". H900 also exhibits excellent smoke,.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Plenco 1501 Polyester, Briquette, Compression Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Plenco 1530 Polyester, Briquette, Injection Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Plenco 6553 Phenolic, Granular, Compression Molded Two-Stage Phenolic. PLENCO 06553 is a phenolic molding compound, formulated specifically for automotive brake pistons. 06553 exhibits excellent dimensional stability, and resistance to brake fluids.. |
|||
Arc Resistance | 190 sec | 190 sec | Tungsten electrode; ASTM D495 |
E-Polymers TEKAMID® TA210L Lubricated PA66, DAM LubricatedInformation provided by E-Polymers Co. Ltd. |
|||
Arc Resistance | 190 sec | 190 sec | Tungsten electrode; ASTM D495 |
E-Polymers TEKAMID® TB110M40 , 40% Mineral Filled PA6, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Cytec EN-2555 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Arc Resistance | 190 sec | 190 sec | IPC TM-650 2.5.1 |
Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System MULTICLAD™ HF represents the next generation low-loss thermoset and prepreg system for high-speed and high-frequency printed circuit boards. This technology combines a low-loss, high reliability t.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 685 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, oil .. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,.. |
|||
Arc Resistance | 190 sec | 190 sec | |
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st.. |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Resinoid 1320 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Resinoid 1322 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Resinoid 1323 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Arc Resistance | 190 sec | 190 sec | ASTM D495 |
Resinoid 1329 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC T40(18)-LS Die Casting Replacement Grade Molding Compound BMC T40(18)-LS is a low shrink compound designed as a direct replacement for aluminum die casting applications. T40(18)-LS is UL recognized. Excellent mechanical properties and dimensional stabili.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi.. |
|||
Arc Resistance | >= 190 sec | >= 190 sec | |
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific .. |