Physical Properties Metric English Comments
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D 792
RTP Company RTP 4011 A (Hot Water Moldable) Polyphthalamide (PPA), Glass Fiber
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
Base Material; ASTM D792
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal
These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at..
Specific Gravity 1.75 - 1.76 g/cc
1.75 - 1.76 g/cc
ASTM D792
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
RTP Company RTP 211G HS  Nylon 4/6 (PA 4/6) Glass Fiber 60% - Heat Stable  (discontinued **)
Glass Fiber 60% - Heat StableComments:Glass FiberHeat Stable(Dry As Molded)Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Infor..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Premix Premi-Glas® 1265 VE 1265-VE (Compression Molded) Glass Reinforced Vinyl Ester TMC  (discontinued **)<
Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti..
Specific Gravity 1.75 g/cc
1.75 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1105-8451 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Specific Gravity 1.75 - 1.85 g/cc
1.75 - 1.85 g/cc
ASTM D792
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Specific Gravity 1.75 - 1.85 g/cc

@Thickness 1.57 mm
1.75 - 1.85 g/cc

@Thickness 0.0620 in
ASTM D792
Industrial Laminates/Norplex NP504 Glass Fabric
Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Haysite HCR-125 Vinyl Ester Sheet, Corrosion Resistant
HCR-125 is a corrosion resistant vinyl ester sheet created by impregnating fiber glass mat, synthetic surface veil, and inert additives with Derkane 470 resin and catalyst. A compression molded pro..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D 792
SABIC Innovative Plastics LNP Lubricomp KFL36XXC Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KFL36 is an Acetal containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Specific Gravity 1.75 g/cc
1.75 g/cc
Silberline Tufflake® 3700
Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE
DescriptionPOLYBATCH® 20232U is a yellow color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability ..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE
DescriptionPOLYBATCH® 20232U is a yellow color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability ..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D 792
RTP Company RTP 205 TFE 15 FR Nylon 6/6 (PA), Glass Fiber - PTFE Lubricated - Flame Retardant
Specific Gravity 1.75 - 1.95 g/cc
1.75 - 1.95 g/cc
IEC 1212-2 7.2
Hippe EP GC 21 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relative ..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant
BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was..
Specific Gravity 1.75 - 2.05 g/cc
1.75 - 2.05 g/cc
Bulk Molding Compounds BMC 606 Mineral Filled, Glass Reinforced Polyester Compound
BMC 606 is a mineral filled, glass reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, excellent impact strength,..
Specific Gravity 1.75 - 1.85 g/cc
1.75 - 1.85 g/cc
Bulk Molding Compounds BMC 840 Corrosion Resistant Molding Compound
BMC 840 is a very high strength, corrosion resistant compound suitable for compression, transfer and stuffer injection molding.Typical applications are pump housings and impellers.
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Asahi Glass F-Clean® Film for Greenhouses
F-CLEAN®, produced by Asahi Glass Company, Ltd., is a Ethylene-Tetrafluoroethylene copolymer (ETFE) film used as the preferred covering material for horticultural greenhouses. High ten..
Specific Gravity 1.75 - 1.77 g/cc
1.75 - 1.77 g/cc
ASTM D792
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Specific Gravity 1.75 - 1.95 g/cc
1.75 - 1.95 g/cc
Bulk Molding Compounds BMC 945 Conductive Grade Bulk Molding Compound
BMC 945 is an ESD level Conductive grade of Bulk Molding Compound and is suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reacti..
Specific Gravity 1.75 - 1.76 g/cc
1.75 - 1.76 g/cc
ASTM D792
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Hylar 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong and ..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
A. Schulman POLYBATCH™ Orange LL10257/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® LL10257/4 is an orange color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® LL10257/4 is he..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D 792
RTP Company RTP 4005.3 FR A HS Polyphthalamide (PPA), Glass Fiber - Flame Retardant - Heat Stabilized