Polymer Property : Specific Gravity = 1.75 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.75 - 1.85 g/cc
1.75 - 1.85 g/cc
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock..
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer
Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie..
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi..
Specific Gravity 1.75 - 2.25 g/cc
1.75 - 2.25 g/cc
ASTM D792
Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer
Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
PolyOne Therma-Tech™ SF-5000C TC Polyphenylene Sulfide (PPS)  (discontinued **)
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm..
Specific Gravity 1.75 g/cc
1.75 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1301-8331 PPS, linear, with glass fiber, thermally conductive modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Coil formers, duty parts in p..
Specific Gravity 1.75 - 1.85 g/cc

@Thickness 1.57 mm
1.75 - 1.85 g/cc

@Thickness 0.0620 in
ASTM D792
Industrial Laminates/Norplex NP504 Glass Fabric
Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note..
Specific Gravity 1.75 - 1.81 g/cc
1.75 - 1.81 g/cc
ASTM D 792
Karina E 801-10/1-J-RT-PO White PVC Compound
PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow 20232U Concentrate Based In LLDPE
DescriptionPOLYBATCH® 20232U is a yellow color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability ..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow 2200 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 2200 is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2200 contai..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D 792
RTP Company RTP 1307 MS 5 Polyphenylene Sulfide (PPS), 40 Glass Fiber-5 Molydisulfide
Specific Gravity 1.75 - 1.95 g/cc
1.75 - 1.95 g/cc
IEC 1212-2 7.2
Hippe EP GC 21 Woven Glass Cloth Reinforced Epoxy Resin - Round, Rolled Tube
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperatures. Very good stability of electrical properties when exposed to high relative ..
Specific Gravity 1.75 - 2.05 g/cc
1.75 - 2.05 g/cc
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound
BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati..
Specific Gravity 1.75 - 1.90 g/cc
1.75 - 1.90 g/cc
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound
BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Asahi Glass Fluon® ETFE Film
Applications: Electronics, Energy Saving, Wallpaper, Sound Suppression Walls, Aviation and SpaceInformation provided by Asahi Glass Company, Inc.
Specific Gravity 1.75 - 1.77 g/cc
1.75 - 1.77 g/cc
ASTM D792
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
Bulk Molding Compounds BMC 1412 Flame and Track Resistant
BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu..
Specific Gravity 1.75 - 2.05 g/cc
1.75 - 2.05 g/cc
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester
BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel..
Specific Gravity 1.75 - 1.85 g/cc
1.75 - 1.85 g/cc
Bulk Molding Compounds BMC 810 General Purpose Molding Compound
BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is wel..
Specific Gravity 1.75 - 1.90 g/cc
1.75 - 1.90 g/cc
Bulk Molding Compounds BMC 900 Thermoset Polyester, Soft Flow Encapsulation Grade
BMC 900 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an..
Specific Gravity 1.75 - 1.95 g/cc
1.75 - 1.95 g/cc
Bulk Molding Compounds BMC 945 Conductive Grade Bulk Molding Compound
BMC 945 is an ESD level Conductive grade of Bulk Molding Compound and is suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reacti..
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 - 1.80 g/cc
1.75 - 1.80 g/cc
ASTM D792
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers.
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
RTP Company RTP 1389 HEC  Polyphenylene Sulfide (PPS) Nickel-Coated Carbon Fiber 50% - EMI/ESD &n
Nickel-Coated Carbon Fiber 50% - EMI/ESDComments:EMI/RFI/ESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can a..
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Solvay Specialty Polymers Xydar® M-345 Liquid Crystal Polymer, 45% Mineral Filled  (discontinued **)
XYDAR M-345 Liquid Crystal Polymer (LCP) is a 45% mineral-filled injection molding grade with exceptional moldability. XYDAR M-345 resin can fill very thin walls over long flow lengths with little o..