BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connectors etc. in household appliance.Information provided by BASF
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Melt Flow 258 g/10 min

@Load 5.00 kg,
Temperature 275 °C
258 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
50 mm/min; ISO 527-1/-2
Elongation at Yield 3.4 %
3.4 %
50 mm/min; ISO 527-1/-2
Modulus of Elasticity 3.60 GPa
522 ksi
ISO 527-1/-2
Flexural Strength 110 MPa
16000 psi
at max force; ISO 178
Flexural Modulus 3.60 GPa
522 ksi
ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
ISO 180/A
3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 7.00 J/cm²

@Temperature 23.0 °C
33.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
9.00 J/cm²

@Temperature -30.0 °C
42.8 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
DIN 53765
Flammability, UL94 V-2

@Thickness >=0.400 mm
V-2

@Thickness >=0.0157 in
Electrical Properties Metric English Comments
Comparative Tracking Index 350 V
350 V
Test solution A; IEC 60112
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Injection-molding/Extrusion
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Injection-molding
Descriptive Properties Value Comments
Color BK 23079
Commercial Status Europe