Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 3.60 GPa | 522 ksi | dry |
Murtfeldt Murylon® 6 Cast Nylon 6 Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | |
Lehmann & Voss LUVOCOM® 1105-7786 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Emergency running property.Improved wear behaviour, low warpage.High chemical resistance p.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | |
Lehmann & Voss LUVOCOM® 1105-7685 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Super.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 18MB090 OPP Film Product Description: Biaxially oriented polypropylene film metallizable on one side, with a slip controlled broad seal range surface on the other side. Once metalized, film designed to be used in la.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 20MB080 OPP Film Product Description: Bicor 20NB080 is a biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a s.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | TD; ExxonMobil Method |
ExxonMobil Bicor™ 29MB080 OPP Film Product Description: A biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a single web in HFFS.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | TD; ExxonMobil Method |
ExxonMobil Label-Lyte™ 29LL210 Preliminary Data Sheet OPP Film Product Description: A biaxially oriented, transparent polypropylene film for pressure sensitive labeling and tape applications.Availability: Africa & Middle East and EuropeKey Features: High yieldG.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM383 OPP Film Product Description: A biaxially oriented very high barrier metalized polypropylene film. This film offers an outstanding moisture barrier and a broad seal range surface on the other side. This film.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM388 OPP Film Product Description: A metallized biaxially oriented polypropylene film, metalized on one side with a broad seal range surface on the other side. This film is designed for high barrier performance p.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM488 OPP Film Product Description: A metalized biaxially oriented polypropylene film, metalized on one side. MM488 is typically used in laminates as the inner web for VFFS and HFFS applications. Due to its slip c.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | TD; ExxonMobil Method |
ExxonMobil Metallyte™ 20MM480 OPP Film Product Description: A metalized biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. It is typically used in lamination with other substrates on HFFS and V.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | ISO 527-1/-2 |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Conditioned) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | ISO 527-1/-2 |
BASF Ultramid® C3U10 BK 23079 PA6/66 FR (Dry) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | ISO 527-1/-2 |
BASF Ultramid® C3U10 PA6/66 FR (Dry) Description: Flame-retardant injection-molding grade; light colorable. Burning behavior optimized for glow-wire requirements of IEC 60335. Typical applications are switches, housings, plug connector.. |
|||
Modulus of Elasticity | 3.60 GPa | 522 ksi | ISO 178 |
Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead Flame retardant, 15% glass bead filled, with halogensInformation provided by Addiplast. |