Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultradur® S 4090 GM13 5/15% Glass/Mineral Filled PBT

Category Polymer , Thermoplastic , ASA Polymer , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + ASA Blend, Glass Fiber Reinforced , Polybutylene Terephthalate (PBT), Mineral Filled
Manufacturer BASF
Trade Name Ultradur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultradur® S 4090 GM13 5/15% Glass/Mineral Filled PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber and 15% mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation grilles and housing covers.Information provided by BASF
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Water Absorption 0.40 %
0.40 %
Saturation; DIN 53495/1L
Moisture Absorption at Equilibrium 0.20 %
0.20 %
23°C; 50% RH
Viscosity Measurement 135
135
[ml/g]; Viscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
Sheet
Linear Mold Shrinkage, Transverse 0.0075 cm/cm
0.0075 in/in
Sheet
Melt Flow 9.59 g/10 min

@Load 2.16 kg,
Temperature 275 °C
9.59 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
50 mm/min; ISO 527-2
Elongation at Break 2.9 %
2.9 %
50mm/min; ISO 527-2
Modulus of Elasticity 5.90 GPa
856 ksi
ISO 527-2
Flexural Strength 115 MPa
16700 psi
ISO 178
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 5.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
2.78 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
Melting Point 220 - 225 °C
428 - 437 °F
DSC; ISO 11357-3
Maximum Service Temperature, Air 170 °C
338 °F
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
ISO 75-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 93
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
IEC 93
Dielectric Constant 4.1

@Frequency 1.00e+6 Hz
4.1

@Frequency 1.00e+6 Hz
IEC 250
Dissipation Factor 0.028

@Frequency 1.00e+6 Hz
0.028

@Frequency 1.00e+6 Hz
IEC 250
Comparative Tracking Index 250 V
250 V
Test solution A; IEC 112
Processing Properties Metric English Comments
Melt Temperature 250 - 275 °C
482 - 527 °F
Injection-molding
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Descriptive Properties Value Comments
Color Black
Commercial Status Europe
Primary Processing Technique Injection Molding
Copyright © lookpolymers.com All Rights Reserved