Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 170 °C | 338 °F | Intermittent |
Nylacast PA6C Cast Nylon 6 Natural PA6 is the base to the other grades of material offered by Nylacast. It is available in Natural (off white) or Black colour. It is made by ionic polymerisation of e-caprolactam under anhydri.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short term |
Polikim KESTAMID® PA6G Polyamide 6 Kestamid® is also known as Cast Polyamide or Cast Nylon. Kestamid® is an engineering plastic used commonly in all industrial branches for its superior mechanical, physical, chemical and electrical.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short term |
Polikim KESTLUB® Polyamide 6 + Lubricant Kestlub® is a special type of cast polyamide ideal for bearings. It is produced by adding lubricants to cast polyamide through special processes. It performs extremely well in bearing applications .. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Deflection Temp.; ASTM D648 |
NCMT NanoPAC™ G2050H High Performance Polypropylene Nanocomposite Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | < 50 h; IEC 60216/T1 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | 20,000 h; IEC 60216/T1 |
Raschig Group RALUPOL® 4385 UP Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Short Time; IEC 60216 |
PolyOne Bergadur™ PB40 G15 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short period, no load |
Omnia Plastica Akulon® PET Arnite Omnialite Arnite is a relatively new semi-crystalline polymer developed for technical applications. It is suitable for mechanical parts which require dimensional stability and a low friction coefficient. Omni.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Continuous |
Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data) Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (l.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short term |
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short term |
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | short term |
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
GEHR Plastics PEI Polyetherimide Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and creep resistance. Its unique torque strength permits the economic.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Intermittent |
Global EPP PA 66E Extruded Polyamide 66 Polyamides, commonly referred to as nylons, are macromolecular, partially crystalline thermoplastics. Their physical properties are mainly determined by the composition and structure of their molecu.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-7743 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Lehmann & Voss LUVOCOM® 1106-8154/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | <20000 hours; IEC 60216-P1 |
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Intermittent |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Dry Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Maximum Service Temperature, Air | 170 °C @Time >=1800 sec |
338 °F @Time >=0.500 hour |
Congo Red; BS 2782 |
Teknor Apex Sinvicomp SFE 3500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Hose; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Continuous Use |
Westlake Plastics Tempalux® Film Made from ULTEM® Polyetherimide Resin High heat deflection and continuous use temperature. Inherent flame resistance. Extremely low NBS smoke evolution & superior limiting oxygen index.Ultem® is a trade name of GE Plastics. Informat.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
Chesterton 622 White Grease Description: Chesterton® 622 White Grease is a pure mineral oil grease with PTFE added designed for applications where a clean, nonstaining, food grade lubricant is required. It is a superior, mult.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Long Term |
Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Continuous use |
Hippe PEI A material with very high mechanical strength and high thermoforming stability which can be used at high temperatures. Distinguished by constant dielectric properties, a wide range of frequency and .. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | Short term |
CENTROPLAST CENTROMID 6 G Polyamide 6 Cast This material has good machinability and can be bonded or welded. Its applications include sliding bearings, hammerheads, and toothed gears.Information provided by CENTROPLAST Engineering Plastics .. |
|||
Maximum Service Temperature, Air | 170 °C | 338 °F | |
BASF Ultradur® S 4090 G6 High Speed 30% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 30% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers.. |