Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.59 - 76.0 g/10 min | 9.59 - 76.0 g/10 min | Average value: 30.0 g/10 min Grade Count:21 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Melt Flow | 9.59 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.59 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Melt Flow | 9.59 g/10 min @Load 2.16 kg, Temperature 275 °C |
9.59 g/10 min @Load 4.76 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultradur® S 4090 GM13 5/15% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber and 15% mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventila.. |
|||
Melt Flow | 9.59 - 58.0 g/10 min | 9.59 - 58.0 g/10 min | Average value: 25.7 g/10 min Grade Count:18 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |