Material Notes:
Easy flowing grade for the injection molding and extrusion of low-taint food packaging.Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Water Absorption 0.10 %
0.10 %
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Linear Mold Shrinkage, Flow 0.0045 cm/cm
0.0045 in/in
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 46.0 MPa
6670 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 3.30 GPa
479 ksi
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
Tensile Creep Modulus, 1000 hours 2200 MPa
319000 psi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
Vicat Softening Point 84.0 °C
183 °F
Flammability, UL94 HB

@Thickness 3.18 mm
HB

@Thickness 0.125 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 2.5

@Frequency 1e+6 Hz
2.5

@Frequency 1e+6 Hz
Dissipation Factor 0.000070

@Frequency 1e+6 Hz
0.000070

@Frequency 1e+6 Hz
0.000090

@Frequency 100 Hz
0.000090

@Frequency 100 Hz
Comparative Tracking Index 375 V
375 V
Users viewing this material also viewed the following: