Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
Polycasa AKRYLON XT PMMA AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT .. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179-1 |
Polycasa XT PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -40.0 °C |
8.09 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.70 - 4.00 J/cm² @Temperature -30.0 - -20.0 °C |
8.09 - 19.0 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 2.78 J/cm² Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL A63 AV15 Nylon 6.6 for injection molding Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -40.0 °C |
8.09 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 KV35 Nylon 6.6 for injection molding, 35% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.70 - 2.00 J/cm² | 8.09 - 9.52 ft-lb/in² | Average value: 1.83 J/cm² Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² - NB | 8.09 ft-lb/in² - NB | Average value: 9.57 J/cm² Grade Count:21 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² - NB | 8.09 ft-lb/in² - NB | Average value: 5.06 J/cm² Grade Count:29 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-8373 Polyamide 46, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Improved fri.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 21-8113 Polyamide 6/6T, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® 378 P G7 35% Glass Filled SAN Description: Glass-reinforced grade with very high stiffness and low thermal coefficient of liner expansion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
Styrolution PS 147F GPPS Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
Styrolution PS 495N HIPS Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.High flowGood balance of toughness and heat resistanceUL 94 HBInfor.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
Styrolution PS 158K GPPS Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature 23.0 °C |
8.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styron TYRILâ„¢ 875 SAN Resin Overview: TYRIL Styrene-actylonitrile (SAN) resins are designed by Styron to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | ISO 179 |
Chi Mei Kibisan® PN-117C SAN High Clarity |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Starpylen HZ 30WF2 PP, 30% Wood Fiber Filled, Injection Molding Starpylen HZ 30WF2 is a 30% Wood Fiber Reinforced Polypropylene Injection Molding Resin (also known as HZ30WF2)Information provided by Eurostar. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | |
BASF Polystyrol® 143 E Polystyrene (Europe) Medium strength, easy flowing general-purpose grade, suitable for blending with impact-modified Polystyrol, Styrolux and as a coextruded glossy capping layer.Data was collected by ISO methods and pr.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | |
BASF Polystyrol® 143 EO Polystyrene (Europe) Easy flowing grade for the injection molding and extrusion of low-taint food packaging.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.70 J/cm² | 8.09 ft-lb/in² | |
BASF Polystyrol® 158 K Polystyrene (Global) Heat-resistant, rapid freezing general-purpose grade. Suitable for expanded film and for blending with Styrolux and impact-modified Polystyrol in heat contact applications (e.g. coffee cups).Data w.. |
|||
Charpy Impact Unnotched | 1.70 J/cm² @Temperature -30.0 °C |
8.09 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1102 J Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.70 - 1.70 J/cm² @Temperature -40.0 - -20.0 °C |
8.09 - 8.09 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.70 J/cm² Grade Count:1 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Charpy Impact Unnotched | 1.70 - 1000 J/cm² | 8.09 - 4760 ft-lb/in² | Average value: 4.44 J/cm² Grade Count:23 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |