Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
Polimeri Europa KOSTIL B266 Styrene Acrylonitrile
Symbol according to ISO 1043-1: SAN Grade designation according to ISO 4894-SAN 2,M,105-15 Standard injection moulding grade with good chemical resistance Application fields: household and small ..
Charpy Impact Unnotched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
Polimeri Europa KOSTIL B266 Styrene Acrylonitrile
Symbol according to ISO 1043-1: SAN Grade designation according to ISO 4894-SAN 2,M,105-15 Standard injection moulding grade with good chemical resistance Application fields: household and small ..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179
Polycasa AKRYLON XT PMMA
AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT ..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179-1
Polycasa XT PMMA
QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
DIN 53453
Nilit FRIANYL B63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.70 - 4.00 J/cm²

@Temperature -30.0 - -20.0 °C
8.09 - 19.0 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 2.78 J/cm² Grade Count:4
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eU
Nilit FRIANYL A63 AV15 Nylon 6.6 for injection molding
Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.70 J/cm²

@Temperature -40.0 °C
8.09 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 KV35 Nylon 6.6 for injection molding, 35% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 1.70 - 2.00 J/cm²
8.09 - 9.52 ft-lb/in²
Average value: 1.83 J/cm² Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Charpy Impact Unnotched 1.70 J/cm² - NB
8.09 ft-lb/in² - NB
Average value: 9.57 J/cm² Grade Count:21
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact Unnotched 1.70 J/cm² - NB
8.09 ft-lb/in² - NB
Average value: 5.06 J/cm² Grade Count:29
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 19-8373 Polyamide 46, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Improved fri..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 20-8149 Polyphthalamide, with carbon fiber and glass fiber, thermally conductive modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 21-8113 Polyamide 6/6T, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-7896 PPS, linear, with carbon fiber, thermally conductive modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Stiff parts, low coefficient of..
Charpy Impact Unnotched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® 378 P G7 35% Glass Filled SAN
Description: Glass-reinforced grade with very high stiffness and low thermal coefficient of liner expansion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179
Styrolution PS 147F GPPS
Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179
Styrolution PS 495N HIPS
Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.High flowGood balance of toughness and heat resistanceUL 94 HBInfor..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179
Styrolution PS 158K GPPS
Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo..
Charpy Impact Unnotched 1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styron TYRILâ„¢ 875 SAN Resin
Overview: TYRIL Styrene-actylonitrile (SAN) resins are designed by Styron to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1fu
Evonik Corporation Plexiglas® XT Grey 99561 RP Extruded Acrylic Sheet
Description: PLEXIGLAS® XT Grey 99561 RP is an extruded acrylic sheet with embedded micro lenses that is developed to act as rear projection screen. The integrated micro lenses perform an excellent..
Charpy Impact Unnotched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eU
Celanese Celanex® 5214HF PBT, 15% Glass Reinforced
Celanex 5214HF is a high flow, 15% glass reinforced, high gloss, flame retardant polyester.Pre-drying: 250F (120C) for 4 HoursInformation provided by Celanese Corporation.
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
BASF Polystyrol® 143 E Polystyrene (Europe)
Medium strength, easy flowing general-purpose grade, suitable for blending with impact-modified Polystyrol, Styrolux and as a coextruded glossy capping layer.Data was collected by ISO methods and pr..
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
BASF Polystyrol® 143 EO Polystyrene (Europe)
Easy flowing grade for the injection molding and extrusion of low-taint food packaging.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
BASF Polystyrol® 158 K Polystyrene (Global)
Heat-resistant, rapid freezing general-purpose grade. Suitable for expanded film and for blending with Styrolux and impact-modified Polystyrol in heat contact applications (e.g. coffee cups).Data w..
Charpy Impact Unnotched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1102 J Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 1.70 - 1.70 J/cm²

@Temperature -40.0 - -20.0 °C
8.09 - 8.09 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 1.70 J/cm² Grade Count:1
Overview of materials for Polypropylene with Glass Fiber + Bead Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max..
Charpy Impact Unnotched 1.70 - 1000 J/cm²
8.09 - 4760 ft-lb/in²
Average value: 4.44 J/cm² Grade Count:23
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Charpy Impact Unnotched 1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese CELANEX 5202 PBT, 15% Glass Reinforced
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..