Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.30 GPa
479 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CM5820 PC+ABS (Asia Pacific)
Cycoloy CM5820 resin is a Mineral Filled Non-FR PC+ABS blend with high impact, high modulus, good chemical resistance & improved surface aesthetic, designed for hand help device chassis that require..
Tensile Modulus 3.30 GPa
479 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® 500R PC (Europe-Africa-Middle East)
LEXAN 500R is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and excellent impact pe..
Tensile Modulus 3.30 GPa
479 ksi
ISO 5271/2
Radici Radilon® S 37FL T Nylon 6
Radilon® S (homopolyamides) are normally used in cast and blown extrusion for the production of packaging films. Radilon® S grades can be extruded to a thickness varying from 20 mm to 100 mm.Appl..
Tensile Modulus 3.30 GPa
479 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer
6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S..
Tensile Modulus 3.30 GPa
479 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
Tensile Modulus 3.30 GPa
479 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific)
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
Tensile Modulus 3.30 GPa
479 ksi
Polycasa Acryl® G 88 E Acrylic
Same as Lucryl G 88, but higher resistance to stress cracking and higher processing viscosity. Used for: extruded protective layer on PVC, ABS and PC for outdoor applications, as well as bath tubs ..
Tensile Modulus 3.30 GPa
479 ksi
ASTM D638
PolyOne Stat-Tech™ PI-10SS/000 Polyetherimide - 10% Stainless Steel Fiber  (discontinued **)
Data provided by PolyOne.
Tensile Modulus 3.30 GPa
479 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Noryl V01505 PPE+HIPS
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Tensile Modulus 3.30 GPa
479 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP IBI16 PA 6/12
LNP LUBRICOMP* IBI16 is a compound based on Nylon 6/12 resin containing 30% Glass Bead, 2% Silicone. Added features of this material include: Wear Resistant.
Tensile Modulus 3.30 GPa
479 ksi
DIN 53457
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Dry
Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH
Tensile Modulus 3.30 GPa
479 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics ULTEM 8015 PEI
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 100/100 with low toxicity, smoke, and flame evolution. ECO Conforming.
Tensile Modulus 3.30 GPa
479 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem UR9076LG PEI
Standard flow mineral filled Polyetherimide Blend. Restricted sales to GE Specialty Film & Sheet.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 3.30 GPa
479 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC
LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable.
Tensile Modulus 3.30 GPa
479 ksi
ISO 527-1/-2
Styrolution Polystyrol 143 E GR 21 PS
Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b..
Tensile Modulus 3.30 GPa
479 ksi
ISO 527-1/-2
Styrolution Polystyrol 158 K GR 2 PS
Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati..
Tensile Modulus 3.30 GPa
479 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP NF001XXX PC+ABS
LNP* THERMOCOMP* PCA-F-1001 is a compound based on PC+ABS resin containing 5% Glass Fiber.
Tensile Modulus 3.30 GPa
479 ksi
ISO 527-1/-2
DSM Stanyl® TE341 Nylon 46 (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Tensile Modulus 3.30 GPa
479 ksi
dry; ISO 527-1/-2
DSM Stanyl® TS300 PA46
Tensile Modulus 3.30 GPa
479 ksi
dry; ISO 527-1/-2
DSM Stanyl® TW341-J PA46
Heat Stabilized, Lubricated
Tensile Modulus 3.30 GPa
479 ksi
dry; ISO 527-1/-2
DSM Stanyl® TW341-N PA46
Heat Stabilized, Lubricated
Tensile Modulus 3.30 GPa
479 ksi
ISO 527-1/-2
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t..
Tensile Modulus 3.30 GPa
479 ksi
ISO 527-1/-2
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..
Tensile Modulus 3.30 GPa
479 ksi
ISO 527-1/-2
DuPont Performance Polymers Delrin® SC690 NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare indus..
Tensile Modulus 3.30 GPa
479 ksi
1 mm/min
Arkema Group Orgalloy® RS 6010 Nylon 6 Alloy, 10% Glass Fiber Reinforced (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties..
Tensile Modulus 3.30 GPa
479 ksi
1 mm/min
Arkema Group Altuglas® GR 7E LIL Acrylic
ALTUGLAS GR 7E LIL is an injection molding grade with excellent balance between mechanical, thermal and optical properties.Key features : easy processing and demolding improved chemical resistance ..
Tensile Modulus 3.30 GPa
479 ksi
BASF Polystyrol® 158 K Polystyrene (Global)
Heat-resistant, rapid freezing general-purpose grade. Suitable for expanded film and for blending with Styrolux and impact-modified Polystyrol in heat contact applications (e.g. coffee cups).Data w..
Tensile Modulus 3.30 GPa

@Temperature 23.0 °C
479 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG311DP is a medium-high viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications ..
Tensile Modulus 3.30 GPa
479 ksi
1 mm/min
Arkema Group Oroglas® V 920 Acrylic, Injection Molding Grade  (discontinued **)
OROGLAS V 920 is an injection molding grade with a good balance of properties :Superior flow with medium thermal resistance.The processing of OROGLAS V 920 is easy in terms of injection molding, mo..
Tensile Modulus 3.30 GPa
479 ksi
1 mm/min
Arkema Group Oroglas® V 920 T Acrylic, Injection Molding Grade  (discontinued **)
OROGLAS V 920 T is an injection molding grade with an improved thermal resistance HDT A ( 1.82 MPa ) = 96°c without any adverse effect on mechanical and optical properties.The processing of OROGLAS..