Material Notes:
Polyether block amide PEBAX® 3533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Water Absorption 1.2 %

@Temperature 23.0 °C,
Time 86400 sec
1.2 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 0.40 %

@Temperature 20.0 °C
0.40 %

@Temperature 68.0 °F
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 4.00 mm,
Time 86400 sec
0.0050 in/in

@Thickness 0.157 in,
Time 24.0 hour
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Thickness 4.00 mm,
Time 86400 sec
0.0080 in/in

@Thickness 0.157 in,
Time 24.0 hour
Mechanical Properties Metric English Comments
Hardness, Shore D 33
33
Instantaneous, Conditioned 15 days at 23°C - 50% RH; ISO 868
25

@Time 15.0 sec
25

@Time 0.00417 hour
Conditioned 15 days at 23°C - 50% RH; ISO 868
Tensile Strength at Break 39.0 MPa
5660 psi
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Elongation at Break >= 600 %
>= 600 %
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Flexural Modulus 0.0210 GPa
3.05 ksi
Conditioned 15 days at 23°C - 50% RH; ISO178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 144 °C
291 °F
ISO 11357
Vicat Softening Point 77.0 °C

@Load 1.02 kg
171 °F

@Load 2.25 lb
ISO 306
Processing Properties Metric English Comments
Processing Temperature 205 °C
401 °F
Recommended Extrusion Temperature
190 - 220 °C
374 - 428 °F
Extrusion Range
Nozzle Temperature 210 °C
410 °F
Recommended
180 - 240 °C
356 - 464 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Drying Temperature 55.0 - 65.0 °C
131 - 149 °F
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour
Users viewing this material also viewed the following: