Material Notes:
Product description: Grivory XE 3996 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO-Polymer designation: PA 10T/X ASTM-Designation: PPA, polyphthalamide The main distinguishing features of Grivory HT-PPA, when compared to other polyamides, are its good performance at high temperatures providing parts which are stiffer, stronger, have better heat distortion and dimensional stability as well as excellent chemical resistance and low moisture absorption. Grivory XE 3996 black 9225 is especially suitable for injection molded components in electrical and electronic applications. The material is suitable for lead-free SMT reflow soldering acc. i.e. JEDEC J-STD-020C (peak temperature 260°C). Components conforming to JEDEC MSL1 are achievable.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Water Absorption 2.0 %
2.0 %
ISO 62
Moisture Absorption 0.800 %
0.800 %
ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 225 MPa
32600 psi
dry; ISO 2039-1
225 MPa
32600 psi
conditioned; ISO 2039-1
Tensile Strength at Break 150 MPa
21800 psi
dry; ISO 527-1/-2
150 MPa
21800 psi
conditioned; ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
dry; ISO 527-1/-2
2.0 %
2.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 9.50 GPa
1380 ksi
conditioned; ISO 527-1/-2
9.50 GPa
1380 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
dry; ISO 179/1eU
4.00 J/cm²
19.0 ft-lb/in²
conditioned; ISO 179/1eU
4.00 J/cm²

@Temperature 30.0 °C
19.0 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
4.00 J/cm²

@Temperature 30.0 °C
19.0 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
dry; ISO 179/1eA
0.700 J/cm²
3.33 ft-lb/in²
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
36.1 µin/in-°F
ISO 11359-1/-2
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °C
302 °F
long term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 140 °C
284 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
dry; IEC 60093
1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 33.0 kV/mm
838 kV/in
dry; IEC 60243-1
33.0 kV/mm
838 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Cooling and climate control
Exterior
Fuel systems
Interior
Powertrain and Chassis
Electricals & Electronics Electrical appliances
Electrical equipment
Energy distribution
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Bio based Polyamide
Hydrolysis resistant
Special Characteristics Improved heat resistance
Improved UV resistance (outdoor use)