Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3010-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3011-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3011-70A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3040-70A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Multibase TPSiV™ 3340-55A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
LATI Latigea B01 F1 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
LATI Latigray 37 B01-01 CX/35 Bio-Polymer Radiopaque compound based on Bio-Polymer (PLA, PHB, ...). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BC142MO Polypropylene Copolymer BC142MO is a controlled rheology polypropylene heterophasic copolymer. It is characterized by high impact strength, good stiffness, excellent process ability, good flow properties and low warpage. .. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BD310MO Polypropylene Copolymer BD310MO is a heterophasic copolymer. This grade is characterized by an optimum combination of good impact strength and very high stiffness. This grade is mildly nucleated to maximize the mechanical.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis BE375MO Polypropylene Copolymer BE375MO is a heterophasic copolymer. This grade is characterized by optimum combination of high impact strength and stiffness. This grade is formulated for an excellent antistatic performance. Elect.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis Bormod™ BJ368MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tec.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis Bormod™ BF970MO Polypropylene for Injection Molding Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | actual surface temp |
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | actual surface temp |
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
RTP Company RTP 2999 X 125934 A NS Polyether-Block-Amide (PEBA / COPA); Barium Sulfate Filled |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar DS1910HF Polymer, Natural Durastar DS1910HF polymer is a high flow grade of Durastar that contains a mold release. Durastar DS1910HF flow lengths are increased 20-40% relative to Durastar DS1010 as shown by spiral flow testi.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN620 Polymer, Natural Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar AN001 Copolyester, Natural Eastar AN001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar AN011 Copolyester Eastar AN011 copolyester is a high flow product. Eastar AN011 flow lengths are increased 20-40% relative to Eastar AN001 as shown by spiral flow testing. Other outstanding features of Eastar are eas.. |
|||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |
Eastman Eastar DN001HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Eastman Eastar MN052 Polyester, Natural Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 2533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 2533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® 3533 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 3533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Arkema Group Pebax® MX 1205 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® MX 1205 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to mee.. |
|||
Mold Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |
Borealis HF136MO Polypropylene HF136MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by a good combination of mechanical and flow properties. This polymer is a CR (controlled rheology.. |